Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 1.21 g/cm³ Show Supplier Material materials with Dichte of 1.21 g/cm³ | dry | ISO 1183 |
Moisture absorption | 2 % Show Supplier Material materials with Moisture absorption of 2 % | dry | Sim. to ISO 62 |
Wasserabsorption | 7.5 % Show Supplier Material materials with Wasserabsorption of 7.5 % | dry | Sim. to ISO 62 |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Dehnung | 4 % Show Supplier Material materials with Dehnung of 4 % | dry | ISO 527-1/-2 | |
50 % Show Supplier Material materials with Dehnung of 50 % | conditioned | ISO 527-1/-2 | ||
Elastizitätsmodul | 1.6 GPa Show Supplier Material materials with Elastizitätsmodul of 1.6 GPa | conditioned | ISO 527-1/-2 | |
4.2 GPa Show Supplier Material materials with Elastizitätsmodul of 4.2 GPa | dry | ISO 527-1/-2 | ||
Elongation at yield | 3 % Show Supplier Material materials with Elongation at yield of 3 % | dry | ISO 527-1/-2 | |
30 % Show Supplier Material materials with Elongation at yield of 30 % | conditioned | ISO 527-1/-2 | ||
Schlagfestigkeit, Charpy gekerbt | -30 °C | 3 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 3 kJ/m² | dry | ISO 179/1eA |
-30 °C | 5 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 5 kJ/m² | conditioned | ISO 179/1eA | |
23 °C | 4 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 4 kJ/m² | dry | ISO 179/1eA | |
23 °C | 9 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 9 kJ/m² | conditioned | ISO 179/1eA | |
Schlagzähigkeit, Charpy ungekerbt | 23 °C | 40 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 40 kJ/m² | dry | ISO 179/1eU |
Thermisch
Property | Value | Condition | Thickness | Testing Standard | Comment |
---|---|---|---|---|---|
Entflammbarkeit | V-2 | dry | 1.5 mm | IEC 60695-11-10 | UL recognition :Yes |
Glow Wire Flammability Index | 960 °C Show Supplier Material materials with Glow Wire Flammability Index of 960 °C | dry | 0.38 mm | IEC 60695-2-12 | |
960 °C Show Supplier Material materials with Glow Wire Flammability Index of 960 °C | dry | 3 mm | IEC 60695-2-12 | ||
Glow Wire Ignition Temperature | 850 °C Show Supplier Material materials with Glow Wire Ignition Temperature of 850 °C | dry | 3 mm | IEC 60695-2-13 | |
930 °C Show Supplier Material materials with Glow Wire Ignition Temperature of 930 °C | dry | 0.38 mm | IEC 60695-2-13 | ||
Relative temperature index, electrical | 150 °C Show Supplier Material materials with Relative temperature index, electrical of 150 °C | dry | 0.38 mm | UL746B | |
Relative temperature index, mechanical impact | 80 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 80 °C | dry | 0.38 mm | UL746B | |
Relative temperature index, mechanical strength | 95 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 95 °C | dry | 0.38 mm | UL746B | |
Schmelzpunkt | 220 °C Show Supplier Material materials with Schmelzpunkt of 220 °C | dry | ISO 11357-1/-3 | 10°C/min |
Elektrisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Dielektrizitätskonstante | 3.2 [-] Show Supplier Material materials with Dielektrizitätskonstante of 3.2 [-] | dry | IEC 62631-2-1 | 1MHz |
3.3 [-] Show Supplier Material materials with Dielektrizitätskonstante of 3.3 [-] | dry | IEC 62631-2-1 | 100Hz | |
3.6 [-] Show Supplier Material materials with Dielektrizitätskonstante of 3.6 [-] | conditioned | IEC 62631-2-1 | 1MHz | |
8 [-] Show Supplier Material materials with Dielektrizitätskonstante of 8 [-] | conditioned | IEC 62631-2-1 | 100Hz | |
Durchschlagfestigkeit | 25 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 25 kV/mm | conditioned | IEC 60243-1 | |
30 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 30 kV/mm | dry | IEC 60243-1 | ||
Kriechstromfestigkeit | 600 V Show Supplier Material materials with Kriechstromfestigkeit of 600 V | dry | IEC 60112 | |
Surface resistivity | 1e+14 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+14 Ω/sq | conditioned | IEC 62631-3-2 | |
Verlustfaktor | 90 [-] Show Supplier Material materials with Verlustfaktor of 90 [-] | dry | IEC 62631-2-1 | 100Hz |
200 [-] Show Supplier Material materials with Verlustfaktor of 200 [-] | dry | IEC 62631-2-1 | 1MHz | |
800 [-] Show Supplier Material materials with Verlustfaktor of 800 [-] | conditioned | IEC 62631-2-1 | 1MHz | |
1250 [-] Show Supplier Material materials with Verlustfaktor of 1250 [-] | conditioned | IEC 62631-2-1 | 100Hz | |
Volume resistivity | 1e+11 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+11 Ω·cm | conditioned | IEC 62631-3-1 | |
1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 62631-3-1 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Certifications | Yellow Card Available |