Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 1.38 g/cm³ Show Supplier Material materials with Dichte of 1.38 g/cm³ | dry | ISO 1183 |
Moisture absorption | 2.1 % Show Supplier Material materials with Moisture absorption of 2.1 % | dry | Sim. to ISO 62 |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Biegemodul | 1.2 GPa Show Supplier Material materials with Biegemodul of 1.2 GPa | conditioned | ISO 178 | |
2.1 GPa Show Supplier Material materials with Biegemodul of 2.1 GPa | dry | ISO 178 | ||
Dehnung | 50 % Show Supplier Material materials with Dehnung of 50 % | dry, conditioned | ISO 527-1/-2 | |
Flexural yield strength | 40 MPa Show Supplier Material materials with Flexural yield strength of 40 MPa | conditioned | ISO 178 | |
70 MPa Show Supplier Material materials with Flexural yield strength of 70 MPa | dry | ISO 178 | ||
Schlagfestigkeit, Charpy gekerbt | 23 °C | 12 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 12 kJ/m² | dry | ISO 179/1eA |
23 °C | 19 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 19 kJ/m² | conditioned | ISO 179/1eA | |
Zugfestigkeit | 33 MPa Show Supplier Material materials with Zugfestigkeit of 33 MPa | conditioned | ISO 527-1/-2 | |
45 MPa Show Supplier Material materials with Zugfestigkeit of 45 MPa | dry | ISO 527-1/-2 |
Thermisch
Property | Value | Condition | Thickness | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|---|
Relative temperature index, electrical | 65 °C Show Supplier Material materials with Relative temperature index, electrical of 65 °C | dry | 0.75 mm | UL746B | ||
Relative temperature index, mechanical impact | 65 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 65 °C | dry | 0.75 mm | UL746B | ||
Relative temperature index, mechanical strength | 65 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 65 °C | dry | 0.75 mm | UL746B | ||
Schmelzpunkt | 220 °C Show Supplier Material materials with Schmelzpunkt of 220 °C | dry | ISO 11357-1/-3 | 10°C/min | ||
Wärmeformbeständigkeitstemperatur | 62 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 62 °C | dry | ISO 75-1/-2 | 2 MPa | ||
155 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 155 °C | dry | ISO 75-1/-2 | 0.45 MPa |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Schmelzmassenflussrate | 230 °C | 4.1 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 4.1 g/10min | dry | ISO 1133 |
Schmelzvolumenflussrate | 230 °C | 3 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 3 cm³/10min | dry | ISO 1133 |
Technological properties
Property | ||
---|---|---|
Certifications | Yellow Card Available |