Allgemein
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Dichte | 1.43 g/cm³ Show Supplier Material materials with Dichte of 1.43 g/cm³ | dry | ISO 1183 | |
Moisture absorption | 2.35 % Show Supplier Material materials with Moisture absorption of 2.35 % | dry | Sim. to ISO 62 | |
Sauerstoffindex | 29.0 % Show Supplier Material materials with Sauerstoffindex of 29.0 % | dry | ISO 4589-1/-2 | |
Wasserabsorption | 2.4 % Show Supplier Material materials with Wasserabsorption of 2.4 % | dry | ISO 62 | at 23°C after 24h |
8.6 % Show Supplier Material materials with Wasserabsorption of 8.6 % | dry | Sim. to ISO 62 |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Biegemodul | 3.2 GPa Show Supplier Material materials with Biegemodul of 3.2 GPa | dry | ISO 178 | |
Dehnung | 7 % Show Supplier Material materials with Dehnung of 7 % | dry | ISO 527-1/-2 | |
Elastizitätsmodul | 3.4 GPa Show Supplier Material materials with Elastizitätsmodul of 3.4 GPa | dry | ISO 527-1/-2 | |
Elongation at yield | 5 % Show Supplier Material materials with Elongation at yield of 5 % | dry | ISO 527-1/-2 | |
Flexural yield strength | 130 MPa Show Supplier Material materials with Flexural yield strength of 130 MPa | dry | ISO 178 | |
Schlagfestigkeit, Charpy gekerbt | -30 °C | 3 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 3 kJ/m² | dry | ISO 179/1eA |
23 °C | 4 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 4 kJ/m² | dry | ISO 179/1eA |
Thermisch
Property | Value | Condition | Thickness | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|---|
Entflammbarkeit | V-0 | dry | 1.5 mm | IEC 60695-11-10 | UL recognition :Yes | |
Glasübergangstemperatur | 75 °C Show Supplier Material materials with Glasübergangstemperatur of 75 °C | dry | ISO 11357-1/-2 | 10°C/min | ||
Koeffizient der thermischen Ausdehnung | 8e-07 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 8e-07 1/K | dry | ISO 11359-1/-2 | Parallel | ||
9e-07 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 9e-07 1/K | dry | ISO 11359-1/-2 | Normal | |||
Schmelzpunkt | 295 °C Show Supplier Material materials with Schmelzpunkt of 295 °C | dry | ISO 11357-1/-3 | 10°C/min | ||
Wärmeformbeständigkeitstemperatur | 190 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 190 °C | dry | ISO 75-1/-2 | 2 MPa |
Elektrisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Dielektrizitätskonstante | 3.5 [-] Show Supplier Material materials with Dielektrizitätskonstante of 3.5 [-] | dry | IEC 62631-2-1 | 1MHz |
3.8 [-] Show Supplier Material materials with Dielektrizitätskonstante of 3.8 [-] | dry | IEC 62631-2-1 | 100Hz | |
4.1 [-] Show Supplier Material materials with Dielektrizitätskonstante of 4.1 [-] | conditioned | IEC 62631-2-1 | 1MHz | |
10 [-] Show Supplier Material materials with Dielektrizitätskonstante of 10 [-] | conditioned | IEC 62631-2-1 | 100Hz | |
Durchschlagfestigkeit | 25 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 25 kV/mm | conditioned | IEC 60243-1 | |
30 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 30 kV/mm | dry | IEC 60243-1 | ||
Kriechstromfestigkeit | 225 V Show Supplier Material materials with Kriechstromfestigkeit of 225 V | dry | IEC 60112 | |
Surface resistivity | 1e+14 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+14 Ω/sq | conditioned | IEC 62631-3-2 | |
Verlustfaktor | 50 [-] Show Supplier Material materials with Verlustfaktor of 50 [-] | dry | IEC 62631-2-1 | 100Hz |
200 [-] Show Supplier Material materials with Verlustfaktor of 200 [-] | dry | IEC 62631-2-1 | 1MHz | |
800 [-] Show Supplier Material materials with Verlustfaktor of 800 [-] | conditioned | IEC 62631-2-1 | 1MHz | |
2800 [-] Show Supplier Material materials with Verlustfaktor of 2800 [-] | conditioned | IEC 62631-2-1 | 100Hz | |
Volume resistivity | 1e+07 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+07 Ω·cm | conditioned | IEC 62631-3-1 | |
1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 62631-3-1 |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Density of melt | 1140 g/cm³ Show Supplier Material materials with Density of melt of 1140 g/cm³ | dry | - | |
Schrumpfung | 1.5 % Show Supplier Material materials with Schrumpfung of 1.5 % | dry | Sim. to ISO 294-4 | Parallel |
1.5 % Show Supplier Material materials with Schrumpfung of 1.5 % | dry | Sim. to ISO 294-4 | Normal | |
Thermal conductivity of melt | 0.24 W/(m·K) Show Supplier Material materials with Thermal conductivity of melt of 0.24 W/(m·K) | dry | - |
Technological properties
Property | ||
---|---|---|
Certifications | Yellow Card Available |