Allgemein
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Dichte | 1.32 g/cm³ Show Supplier Material materials with Dichte of 1.32 g/cm³ | dry | ISO 1183 | |
Moisture absorption | 2.6 % Show Supplier Material materials with Moisture absorption of 2.6 % | dry | Sim. to ISO 62 | |
Wasserabsorption | 2.65 % Show Supplier Material materials with Wasserabsorption of 2.65 % | dry | ISO 62 | at 23°C after 24h |
9.5 % Show Supplier Material materials with Wasserabsorption of 9.5 % | dry | Sim. to ISO 62 |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Biegemodul | 5.8 GPa Show Supplier Material materials with Biegemodul of 5.8 GPa | conditioned | ISO 178 | |
12 GPa Show Supplier Material materials with Biegemodul of 12 GPa | dry | ISO 178 | ||
120 °C | 6.3 GPa Show Supplier Material materials with Biegemodul of 6.3 GPa | dry | ISO 178 | |
160 °C | 5.9 GPa Show Supplier Material materials with Biegemodul of 5.9 GPa | dry | ISO 178 | |
Dehnung | 2.1 % Show Supplier Material materials with Dehnung of 2.1 % | dry | ISO 527-1/-2 | |
5 % Show Supplier Material materials with Dehnung of 5 % | conditioned | ISO 527-1/-2 | ||
120 °C | 5 % Show Supplier Material materials with Dehnung of 5 % | dry | ISO 527-1/-2 | |
160 °C | 5 % Show Supplier Material materials with Dehnung of 5 % | dry | ISO 527-1/-2 | |
180 °C | 5 % Show Supplier Material materials with Dehnung of 5 % | dry | ISO 527-1/-2 | |
200 °C | 5 % Show Supplier Material materials with Dehnung of 5 % | dry | ISO 527-1/-2 | |
Elastizitätsmodul | -40 °C | 13.5 GPa Show Supplier Material materials with Elastizitätsmodul of 13.5 GPa | dry | ISO 527-1/-2 |
6.7 GPa Show Supplier Material materials with Elastizitätsmodul of 6.7 GPa | conditioned | ISO 527-1/-2 | ||
13.5 GPa Show Supplier Material materials with Elastizitätsmodul of 13.5 GPa | dry | ISO 527-1/-2 | ||
120 °C | 6.3 GPa Show Supplier Material materials with Elastizitätsmodul of 6.3 GPa | dry | ISO 527-1/-2 | |
160 °C | 5.7 GPa Show Supplier Material materials with Elastizitätsmodul of 5.7 GPa | dry | ISO 527-1/-2 | |
180 °C | 5.4 GPa Show Supplier Material materials with Elastizitätsmodul of 5.4 GPa | dry | ISO 527-1/-2 | |
200 °C | 5.1 GPa Show Supplier Material materials with Elastizitätsmodul of 5.1 GPa | dry | ISO 527-1/-2 | |
Flexural yield strength | 150 MPa Show Supplier Material materials with Flexural yield strength of 150 MPa | conditioned | ISO 178 | |
280 MPa Show Supplier Material materials with Flexural yield strength of 280 MPa | dry | ISO 178 | ||
120 °C | 150 MPa Show Supplier Material materials with Flexural yield strength of 150 MPa | dry | ISO 178 | |
160 °C | 120 MPa Show Supplier Material materials with Flexural yield strength of 120 MPa | dry | ISO 178 | |
Schlagfestigkeit, Charpy gekerbt | -30 °C | 4.5 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 4.5 kJ/m² | conditioned | ISO 179/1eA |
-30 °C | 5 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 5 kJ/m² | dry | ISO 179/1eA | |
23 °C | 6 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 6 kJ/m² | dry | ISO 179/1eA | |
23 °C | 12 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 12 kJ/m² | conditioned | ISO 179/1eA | |
Schlagzähigkeit, Charpy ungekerbt | -30 °C | 45 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 45 kJ/m² | dry, conditioned | ISO 179/1eU |
23 °C | 50 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 50 kJ/m² | dry | ISO 179/1eU | |
23 °C | 57.0 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 57.0 kJ/m² | conditioned | ISO 179/1eU | |
Zugfestigkeit | -40 °C | 230 MPa Show Supplier Material materials with Zugfestigkeit of 230 MPa | dry | ISO 527-1/-2 |
120 MPa Show Supplier Material materials with Zugfestigkeit of 120 MPa | conditioned | ISO 527-1/-2 | ||
195 MPa Show Supplier Material materials with Zugfestigkeit of 195 MPa | dry | ISO 527-1/-2 | ||
120 °C | 108 MPa Show Supplier Material materials with Zugfestigkeit of 108 MPa | dry | ISO 527-1/-2 | |
160 °C | 92 MPa Show Supplier Material materials with Zugfestigkeit of 92 MPa | dry | ISO 527-1/-2 | |
180 °C | 84 MPa Show Supplier Material materials with Zugfestigkeit of 84 MPa | dry | ISO 527-1/-2 | |
200 °C | 76 MPa Show Supplier Material materials with Zugfestigkeit of 76 MPa | dry | ISO 527-1/-2 |
Thermisch
Property | Value | Condition | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|
Glasübergangstemperatur | 75 °C Show Supplier Material materials with Glasübergangstemperatur of 75 °C | dry | ISO 11357-1/-2 | 10°C/min | |
Koeffizient der thermischen Ausdehnung | 2.5e-07 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 2.5e-07 1/K | dry | ISO 11359-1/-2 | Parallel | |
5e-07 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 5e-07 1/K | dry | ISO 11359-1/-2 | Normal | ||
Schmelzpunkt | 295 °C Show Supplier Material materials with Schmelzpunkt of 295 °C | dry | ISO 11357-1/-3 | 10°C/min | |
Wärmeformbeständigkeitstemperatur | 290 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 290 °C | dry | ISO 75-1/-2 | 2 MPa |
Elektrisch
Property | Value | Condition | Testing Standard |
---|---|---|---|
Volume resistivity | 100000 Ω·cm Show Supplier Material materials with Volume resistivity of 100000 Ω·cm | dry | IEC 62631-3-1 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Automotive Bearing Cages, Gears, Electronic throttle control actuators, Exhaust gas recirculation actuators, Turbo actuators, Coolant valve actuators | |
Certifications | Yellow Card Available | |
Fillers | 15% Carbon Fiber and PTFE |