Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 1.63 g/cm³ Show Supplier Material materials with Dichte of 1.63 g/cm³ | dry | ISO 1183 |
Moisture absorption | 0.9 % Show Supplier Material materials with Moisture absorption of 0.9 % | dry | Sim. to ISO 62 |
Wasserabsorption | 4.1 % Show Supplier Material materials with Wasserabsorption of 4.1 % | dry | Sim. to ISO 62 |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Dehnung | 0.6 % Show Supplier Material materials with Dehnung of 0.6 % | dry | ISO 527-1/-2 | |
Elastizitätsmodul | 12.5 GPa Show Supplier Material materials with Elastizitätsmodul of 12.5 GPa | dry | ISO 527-1/-2 | |
Schlagfestigkeit, Charpy gekerbt | 23 °C | 2 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 2 kJ/m² | dry | ISO 179/1eA |
Zugfestigkeit | 55.0 MPa Show Supplier Material materials with Zugfestigkeit of 55.0 MPa | dry | ISO 527-1/-2 |
Thermisch
Property | Value | Condition | Thickness | Testing Standard | Comment |
---|---|---|---|---|---|
Entflammbarkeit | V-0 | dry | 1.5 mm | IEC 60695-11-10 | UL recognition :Yes |
5VA | dry | 1.6 mm | IEC 60695-11-20 | ||
Glow Wire Flammability Index | 960 °C Show Supplier Material materials with Glow Wire Flammability Index of 960 °C | dry | 0.75 mm | IEC 60695-2-12 | |
960 °C Show Supplier Material materials with Glow Wire Flammability Index of 960 °C | dry | 3 mm | IEC 60695-2-12 | ||
Glow Wire Ignition Temperature | 825 °C Show Supplier Material materials with Glow Wire Ignition Temperature of 825 °C | dry | 0.75 mm | IEC 60695-2-13 | |
900 °C Show Supplier Material materials with Glow Wire Ignition Temperature of 900 °C | dry | 3 mm | IEC 60695-2-13 | ||
Koeffizient der thermischen Ausdehnung | 2.5e-07 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 2.5e-07 1/K | dry | ISO 11359-1/-2 | Parallel | |
2.5e-07 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 2.5e-07 1/K | dry | ISO 11359-1/-2 | Normal | ||
Relative temperature index, electrical | 140 °C Show Supplier Material materials with Relative temperature index, electrical of 140 °C | dry | 0.75 mm | UL746B | |
Relative temperature index, mechanical impact | 110 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 110 °C | dry | 0.75 mm | UL746B | |
Relative temperature index, mechanical strength | 120 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 120 °C | dry | 0.75 mm | UL746B | |
Wärmeleitfähigkeit | 1 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 1 W/(m·K) | dry | ASTM E1461 | through plane | |
8 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 8 W/(m·K) | dry | ASTM E1461 | in plane |
Elektrisch
Property | Value | Condition | Testing Standard |
---|---|---|---|
Durchschlagfestigkeit | 30 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 30 kV/mm | dry | IEC 60243-1 |
Kriechstromfestigkeit | 600 V Show Supplier Material materials with Kriechstromfestigkeit of 600 V | dry | IEC 60112 |
Surface resistivity | 1e+13 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+13 Ω/sq | conditioned | IEC 62631-3-2 |
Volume resistivity | 1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 62631-3-1 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Heat Sinks in LED Lamps | |