Allgemein
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Dichte | 1.18 g/cm³ Show Supplier Material materials with Dichte of 1.18 g/cm³ | dry | ISO 1183 | |
Moisture absorption | 3.7 % Show Supplier Material materials with Moisture absorption of 3.7 % | dry | Sim. to ISO 62 | |
Sauerstoffindex | 27 % Show Supplier Material materials with Sauerstoffindex of 27 % | dry | ISO 4589-1/-2 | |
Wasserabsorption | 3.8 % Show Supplier Material materials with Wasserabsorption of 3.8 % | dry | ISO 62 | at 23°C after 24h |
13.5 % Show Supplier Material materials with Wasserabsorption of 13.5 % | dry | Sim. to ISO 62 |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Biegemodul | 0.9 GPa Show Supplier Material materials with Biegemodul of 0.9 GPa | conditioned | ISO 178 | |
3 GPa Show Supplier Material materials with Biegemodul of 3 GPa | dry | ISO 178 | ||
120 °C | 0.8 GPa Show Supplier Material materials with Biegemodul of 0.8 GPa | dry | ISO 178 | |
160 °C | 0.6 GPa Show Supplier Material materials with Biegemodul of 0.6 GPa | dry | ISO 178 | |
Dehnung | 40 % Show Supplier Material materials with Dehnung of 40 % | dry | ISO 527-1/-2 | |
50 % Show Supplier Material materials with Dehnung of 50 % | conditioned | ISO 527-1/-2 | ||
120 °C | 50 % Show Supplier Material materials with Dehnung of 50 % | dry | ISO 527-1/-2 | |
160 °C | 50 % Show Supplier Material materials with Dehnung of 50 % | dry | ISO 527-1/-2 | |
180 °C | 50 % Show Supplier Material materials with Dehnung of 50 % | dry | ISO 527-1/-2 | |
200 °C | 50 % Show Supplier Material materials with Dehnung of 50 % | dry | ISO 527-1/-2 | |
Elastizitätsmodul | 1 GPa Show Supplier Material materials with Elastizitätsmodul of 1 GPa | conditioned | ISO 527-1/-2 | |
3.3 GPa Show Supplier Material materials with Elastizitätsmodul of 3.3 GPa | dry | ISO 527-1/-2 | ||
120 °C | 0.8 GPa Show Supplier Material materials with Elastizitätsmodul of 0.8 GPa | dry | ISO 527-1/-2 | |
160 °C | 0.65 GPa Show Supplier Material materials with Elastizitätsmodul of 0.65 GPa | dry | ISO 527-1/-2 | |
180 °C | 0.6 GPa Show Supplier Material materials with Elastizitätsmodul of 0.6 GPa | dry | ISO 527-1/-2 | |
200 °C | 0.5 GPa Show Supplier Material materials with Elastizitätsmodul of 0.5 GPa | dry | ISO 527-1/-2 | |
Elongation at yield | 10 % Show Supplier Material materials with Elongation at yield of 10 % | dry | ISO 527-1/-2 | |
20 % Show Supplier Material materials with Elongation at yield of 20 % | conditioned | ISO 527-1/-2 | ||
Flexural yield strength | 50 MPa Show Supplier Material materials with Flexural yield strength of 50 MPa | conditioned | ISO 178 | |
150 MPa Show Supplier Material materials with Flexural yield strength of 150 MPa | dry | ISO 178 | ||
120 °C | 50 MPa Show Supplier Material materials with Flexural yield strength of 50 MPa | dry | ISO 178 | |
160 °C | 40 MPa Show Supplier Material materials with Flexural yield strength of 40 MPa | dry | ISO 178 | |
Schlagfestigkeit, Charpy gekerbt | -30 °C | 4 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 4 kJ/m² | dry, conditioned | ISO 179/1eA |
23 °C | 10 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 10 kJ/m² | dry | ISO 179/1eA | |
23 °C | 35 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 35 kJ/m² | conditioned | ISO 179/1eA | |
Streckgrenze | 55.0 MPa Show Supplier Material materials with Streckgrenze of 55.0 MPa | conditioned | ISO 527-1/-2 | |
100 MPa Show Supplier Material materials with Streckgrenze of 100 MPa | dry | ISO 527-1/-2 | ||
120 °C | 50 MPa Show Supplier Material materials with Streckgrenze of 50 MPa | dry | ISO 527-1/-2 | |
160 °C | 40 MPa Show Supplier Material materials with Streckgrenze of 40 MPa | dry | ISO 527-1/-2 | |
180 °C | 35 MPa Show Supplier Material materials with Streckgrenze of 35 MPa | dry | ISO 527-1/-2 | |
200 °C | 30 MPa Show Supplier Material materials with Streckgrenze of 30 MPa | dry | ISO 527-1/-2 |
Thermisch
Property | Value | Condition | Thickness | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|---|
Entflammbarkeit | V-2 | dry | 1.5 mm | IEC 60695-11-10 | UL recognition :Yes | |
Glasübergangstemperatur | 75 °C Show Supplier Material materials with Glasübergangstemperatur of 75 °C | dry | ISO 11357-1/-2 | 10°C/min | ||
Koeffizient der thermischen Ausdehnung | 8.5e-07 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 8.5e-07 1/K | dry | ISO 11359-1/-2 | Parallel | ||
1.1e-06 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.1e-06 1/K | dry | ISO 11359-1/-2 | Normal | |||
Relative temperature index, electrical | 130 °C Show Supplier Material materials with Relative temperature index, electrical of 130 °C | dry | 0.75 mm | UL746B | ||
Schmelzpunkt | 295 °C Show Supplier Material materials with Schmelzpunkt of 295 °C | dry | ISO 11357-1/-3 | 10°C/min | ||
Temperaturleitfähigkeit | 9.11e-08 mm²/s Show Supplier Material materials with Temperaturleitfähigkeit of 9.11e-08 mm²/s | dry | - | |||
Vicat-Erweichungstemperatur | 290 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 290 °C | dry | ISO 306 | 50°C/h 50N | ||
Wärmeformbeständigkeitstemperatur | 190 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 190 °C | dry | ISO 75-1/-2 | 2 MPa | ||
280 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 280 °C | dry | ISO 75-1/-2 | 0.45 MPa |
Elektrisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Dielektrizitätskonstante | 3.6 [-] Show Supplier Material materials with Dielektrizitätskonstante of 3.6 [-] | dry | IEC 62631-2-1 | 1MHz |
4 [-] Show Supplier Material materials with Dielektrizitätskonstante of 4 [-] | dry | IEC 62631-2-1 | 100Hz | |
4.3 [-] Show Supplier Material materials with Dielektrizitätskonstante of 4.3 [-] | conditioned | IEC 62631-2-1 | 1MHz | |
13 [-] Show Supplier Material materials with Dielektrizitätskonstante of 13 [-] | conditioned | IEC 62631-2-1 | 100Hz | |
Durchschlagfestigkeit | 20 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 20 kV/mm | conditioned | IEC 60243-1 | |
25 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 25 kV/mm | dry | IEC 60243-1 | ||
Kriechstromfestigkeit | 600 V Show Supplier Material materials with Kriechstromfestigkeit of 600 V | dry | IEC 60112 | |
Surface resistivity | 1e+14 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+14 Ω/sq | conditioned | IEC 62631-3-2 | |
Verlustfaktor | 70 [-] Show Supplier Material materials with Verlustfaktor of 70 [-] | dry | IEC 62631-2-1 | 100Hz |
260 [-] Show Supplier Material materials with Verlustfaktor of 260 [-] | dry | IEC 62631-2-1 | 1MHz | |
1000 [-] Show Supplier Material materials with Verlustfaktor of 1000 [-] | conditioned | IEC 62631-2-1 | 1MHz | |
1400 [-] Show Supplier Material materials with Verlustfaktor of 1400 [-] | conditioned | IEC 62631-2-1 | 100Hz | |
Volume resistivity | 1e+10 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+10 Ω·cm | conditioned | IEC 62631-3-1 | |
1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 62631-3-1 |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Density of melt | 987 g/cm³ Show Supplier Material materials with Density of melt of 987 g/cm³ | dry | - | |
Schrumpfung | 2 % Show Supplier Material materials with Schrumpfung of 2 % | dry | Sim. to ISO 294-4 | Parallel |
2 % Show Supplier Material materials with Schrumpfung of 2 % | dry | Sim. to ISO 294-4 | Normal | |
Specific heat capacity melt | 2790.0 J/(kg·K) Show Supplier Material materials with Specific heat capacity melt of 2790.0 J/(kg·K) | dry | - | |
Spiral flow length | 110 | dry | - | 1.0 mm 800 bar |
120 | dry | - | 1.0 mm 900 bar | |
130 | dry | - | 1.0 mm 1000 bar | |
60 | dry | - | 0.5mm 1200 bar | |
70 | dry | - | 0.5mm 1600 bar | |
90 | dry | - | 0.5mm 2000 bar | |
Thermal conductivity of melt | 0.261 W/(m·K) Show Supplier Material materials with Thermal conductivity of melt of 0.261 W/(m·K) | dry | - | |
Viscosity number | 185 cm³/gr Show Supplier Material materials with Viscosity number of 185 cm³/gr | dry | ISO 307, 1157, 1628 |
Technological properties
Property | ||
---|---|---|
Certifications | Yellow Card Available |