Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 1.14 g/cm³ Show Supplier Material materials with Dichte of 1.14 g/cm³ | dry | ISO 1183 |
Moisture absorption | 2.5 % Show Supplier Material materials with Moisture absorption of 2.5 % | dry | Sim. to ISO 62 |
Wasserabsorption | 9 % Show Supplier Material materials with Wasserabsorption of 9 % | dry | Sim. to ISO 62 |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Dehnung | 14.0 % Show Supplier Material materials with Dehnung of 14.0 % | dry | ISO 527-1/-2 | |
Elastizitätsmodul | 3 GPa Show Supplier Material materials with Elastizitätsmodul of 3 GPa | dry | ISO 527-1/-2 | |
Elongation at yield | 3 % Show Supplier Material materials with Elongation at yield of 3 % | dry | ISO 527-1/-2 | |
Schlagfestigkeit, Charpy gekerbt | 23 °C | 6 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 6 kJ/m² | dry | ISO 179/1eA |
Thermisch
Property | Value | Condition | Testing Standard | Thickness | Pressure | Comment |
---|---|---|---|---|---|---|
Ball pressure temperature | 180 °C Show Supplier Material materials with Ball pressure temperature of 180 °C | dry | IEC 60695-10-2 | |||
Glow Wire Flammability Index | 675 °C Show Supplier Material materials with Glow Wire Flammability Index of 675 °C | dry | IEC 60695-2-12 | 3 mm | ||
725 °C Show Supplier Material materials with Glow Wire Flammability Index of 725 °C | dry | IEC 60695-2-12 | 0.75 mm | |||
Schmelzpunkt | 220 °C Show Supplier Material materials with Schmelzpunkt of 220 °C | dry | ISO 11357-1/-3 | 10°C/min | ||
Wärmeformbeständigkeitstemperatur | 60 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 60 °C | dry | ISO 75-1/-2 | 2 MPa | ||
150 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 150 °C | dry | ISO 75-1/-2 | 0.45 MPa |
Elektrisch
Property | Value | Condition | Testing Standard |
---|---|---|---|
Kriechstromfestigkeit | 575 V Show Supplier Material materials with Kriechstromfestigkeit of 575 V | dry | IEC 60112 |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Schmelzvolumenflussrate | 235 °C | 90 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 90 cm³/10min | dry | ISO 1133 | |
Schrumpfung | 1.1 % Show Supplier Material materials with Schrumpfung of 1.1 % | dry | ISO 294-4 | Parallel | |
1.1 % Show Supplier Material materials with Schrumpfung of 1.1 % | dry | ISO 294-4 | Normal |
Technological properties
Property | ||
---|---|---|
Application areas | Surfboard components |