Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 1.29 g/cm³ Show Supplier Material materials with Dichte of 1.29 g/cm³ | dry | ISO 1183 |
Moisture absorption | 0.25 % Show Supplier Material materials with Moisture absorption of 0.25 % | dry | Sim. to ISO 62 |
Wasserabsorption | 0.55 % Show Supplier Material materials with Wasserabsorption of 0.55 % | dry | Sim. to ISO 62 |
Mechanisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Biegemodul | 0.9 GPa Show Supplier Material materials with Biegemodul of 0.9 GPa | dry | ISO 178 | |
Elastizitätsmodul | 1 GPa Show Supplier Material materials with Elastizitätsmodul of 1 GPa | dry | ISO 527-1/-2 | |
Elongation at yield | 18 % Show Supplier Material materials with Elongation at yield of 18 % | dry | ISO 527-1/-2 | |
Härte, Shore D | 56.0 [-] Show Supplier Material materials with Härte, Shore D of 56.0 [-] | dry | ISO 868 | 15s |
Zugfestigkeit | 18 MPa Show Supplier Material materials with Zugfestigkeit of 18 MPa | dry | ISO 527-1/-2 |
Thermisch
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Schmelzmassenflussrate | 230 °C | 24 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 24 g/10min | dry | ISO 1133 |
Technological properties
Property | ||
---|---|---|
Application areas | Chair Carriers, Seat Suspension/Fabrics | |
Fillers | Glass Fiber |