Allgemein
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Dichte | 1.43 g/cm³ Show Supplier Material materials with Dichte of 1.43 g/cm³ | dry | ISO 1183 | |
Moisture absorption | 1.6 % Show Supplier Material materials with Moisture absorption of 1.6 % | dry | Sim. to ISO 62 | |
Wasserabsorption | 1 % Show Supplier Material materials with Wasserabsorption of 1 % | dry | ISO 62 | at 23°C after 24h |
4.9 % Show Supplier Material materials with Wasserabsorption of 4.9 % | dry | Sim. to ISO 62 |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard | Thickness | Comment |
---|---|---|---|---|---|---|
Biegemodul | 7.5 GPa Show Supplier Material materials with Biegemodul of 7.5 GPa | conditioned | ISO 178 | |||
11.5 GPa Show Supplier Material materials with Biegemodul of 11.5 GPa | dry | ISO 178 | ||||
120 °C | 5.8 GPa Show Supplier Material materials with Biegemodul of 5.8 GPa | dry | ISO 178 | |||
160 °C | 5.0 GPa Show Supplier Material materials with Biegemodul of 5.0 GPa | dry | ISO 178 | |||
Dehnung | -40 °C | 3 % Show Supplier Material materials with Dehnung of 3 % | dry | ISO 527-1/-2 | ||
2.7 % Show Supplier Material materials with Dehnung of 2.7 % | dry | ISO 527-1/-2 | 1 mm | |||
3 % Show Supplier Material materials with Dehnung of 3 % | dry | ISO 527-1/-2 | ||||
3.4 % Show Supplier Material materials with Dehnung of 3.4 % | conditioned | ISO 527-1/-2 | ||||
4.3 % Show Supplier Material materials with Dehnung of 4.3 % | conditioned | ISO 527-1/-2 | ||||
120 °C | 5.4 % Show Supplier Material materials with Dehnung of 5.4 % | dry | ISO 527-1/-2 | |||
140 °C | 5.7 % Show Supplier Material materials with Dehnung of 5.7 % | dry | ISO 527-1/-2 | |||
160 °C | 6 % Show Supplier Material materials with Dehnung of 6 % | dry | ISO 527-1/-2 | |||
Elastizitätsmodul | -40 °C | 1.1 GPa Show Supplier Material materials with Elastizitätsmodul of 1.1 GPa | dry | ISO 527-1/-2 | ||
7.9 GPa Show Supplier Material materials with Elastizitätsmodul of 7.9 GPa | conditioned | ISO 527-1/-2 | ||||
8.6 GPa Show Supplier Material materials with Elastizitätsmodul of 8.6 GPa | conditioned | ISO 527-1/-2 | ||||
11 GPa Show Supplier Material materials with Elastizitätsmodul of 11 GPa | dry | ISO 527-1/-2 | ||||
11.5 GPa Show Supplier Material materials with Elastizitätsmodul of 11.5 GPa | dry | ISO 527-1/-2 | 1 mm | |||
100 °C | 5.8 GPa Show Supplier Material materials with Elastizitätsmodul of 5.8 GPa | dry | ISO 527-1/-2 | |||
120 °C | 5.3 GPa Show Supplier Material materials with Elastizitätsmodul of 5.3 GPa | dry | ISO 527-1/-2 | |||
140 °C | 4.8 GPa Show Supplier Material materials with Elastizitätsmodul of 4.8 GPa | dry | ISO 527-1/-2 | |||
160 °C | 4.6 GPa Show Supplier Material materials with Elastizitätsmodul of 4.6 GPa | dry | ISO 527-1/-2 | |||
Flexural yield strength | 180 MPa Show Supplier Material materials with Flexural yield strength of 180 MPa | conditioned | ISO 178 | |||
240 MPa Show Supplier Material materials with Flexural yield strength of 240 MPa | dry | ISO 178 | ||||
120 °C | 120 MPa Show Supplier Material materials with Flexural yield strength of 120 MPa | dry | ISO 178 | |||
160 °C | 100 MPa Show Supplier Material materials with Flexural yield strength of 100 MPa | dry | ISO 178 | |||
Schlagfestigkeit, Charpy gekerbt | -30 °C | 10 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 10 kJ/m² | dry, conditioned | ISO 179/1eA | ||
23 °C | 10 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 10 kJ/m² | dry, conditioned | ISO 179/1eA | |||
Schlagzähigkeit, Charpy ungekerbt | -30 °C | 48 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 48 kJ/m² | conditioned | ISO 179/1eU | ||
-30 °C | 50 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 50 kJ/m² | dry | ISO 179/1eU | |||
23 °C | 62 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 62 kJ/m² | conditioned | ISO 179/1eU | |||
23 °C | 68 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 68 kJ/m² | dry | ISO 179/1eU | |||
Zugfestigkeit | -40 °C | 200 MPa Show Supplier Material materials with Zugfestigkeit of 200 MPa | dry | ISO 527-1/-2 | ||
100 MPa Show Supplier Material materials with Zugfestigkeit of 100 MPa | conditioned | ISO 527-1/-2 | at low thickness | |||
120 MPa Show Supplier Material materials with Zugfestigkeit of 120 MPa | conditioned | ISO 527-1/-2 | ||||
145 MPa Show Supplier Material materials with Zugfestigkeit of 145 MPa | dry | ISO 527-1/-2 | 1 mm | at low thickness | ||
155 MPa Show Supplier Material materials with Zugfestigkeit of 155 MPa | dry | ISO 527-1/-2 | ||||
100 °C | 87 MPa Show Supplier Material materials with Zugfestigkeit of 87 MPa | dry | ISO 527-1/-2 | |||
120 °C | 79 MPa Show Supplier Material materials with Zugfestigkeit of 79 MPa | dry | ISO 527-1/-2 | |||
140 °C | 72 MPa Show Supplier Material materials with Zugfestigkeit of 72 MPa | dry | ISO 527-1/-2 | |||
160 °C | 66 MPa Show Supplier Material materials with Zugfestigkeit of 66 MPa | dry | ISO 527-1/-2 |
Thermisch
Property | Value | Condition | Testing Standard | Thickness | Pressure | Comment |
---|---|---|---|---|---|---|
Ball pressure temperature | 255 °C Show Supplier Material materials with Ball pressure temperature of 255 °C | dry | IEC 60695-10-2 | |||
Entflammbarkeit | V-0 | dry | IEC 60695-11-10 | 1.5 mm | UL recognition :Yes | |
Glasübergangstemperatur | 60 °C Show Supplier Material materials with Glasübergangstemperatur of 60 °C | dry | ISO 11357-1/-2 | 10°C/min | ||
Glow Wire Flammability Index | 960 °C Show Supplier Material materials with Glow Wire Flammability Index of 960 °C | dry | IEC 60695-2-12 | 0.4 mm | ||
960 °C Show Supplier Material materials with Glow Wire Flammability Index of 960 °C | dry | IEC 60695-2-12 | 3 mm | |||
Glow Wire Ignition Temperature | 800 °C Show Supplier Material materials with Glow Wire Ignition Temperature of 800 °C | dry | IEC 60695-2-13 | 0.4 mm | ||
825 °C Show Supplier Material materials with Glow Wire Ignition Temperature of 825 °C | dry | IEC 60695-2-13 | 3 mm | |||
Koeffizient der thermischen Ausdehnung | 2.1e-07 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 2.1e-07 1/K | dry | ISO 11359-1/-2 | Parallel | ||
6.7e-07 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 6.7e-07 1/K | dry | ISO 11359-1/-2 | Normal | |||
Schmelzpunkt | 260 °C Show Supplier Material materials with Schmelzpunkt of 260 °C | dry | ISO 11357-1/-3 | 10°C/min | ||
Wärmeformbeständigkeitstemperatur | 247 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 247 °C | dry | ISO 75-1/-2 | 2 MPa |
Elektrisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Dielektrizitätskonstante | 3.6 [-] Show Supplier Material materials with Dielektrizitätskonstante of 3.6 [-] | dry | IEC 60250 | 1GHz |
3.7 [-] Show Supplier Material materials with Dielektrizitätskonstante of 3.7 [-] | conditioned | IEC 60250 | 1GHz | |
3.9 [-] Show Supplier Material materials with Dielektrizitätskonstante of 3.9 [-] | dry | IEC 62631-2-1 | 1MHz | |
4.2 [-] Show Supplier Material materials with Dielektrizitätskonstante of 4.2 [-] | dry | IEC 62631-2-1 | 100Hz | |
4.3 [-] Show Supplier Material materials with Dielektrizitätskonstante of 4.3 [-] | conditioned | IEC 62631-2-1 | 1MHz | |
7.3 [-] Show Supplier Material materials with Dielektrizitätskonstante of 7.3 [-] | conditioned | IEC 62631-2-1 | 100Hz | |
Durchschlagfestigkeit | 38 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 38 kV/mm | conditioned | IEC 60243-1 | |
41 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 41 kV/mm | dry | IEC 60243-1 | ||
Kriechstromfestigkeit | 600 V Show Supplier Material materials with Kriechstromfestigkeit of 600 V | dry | IEC 60112 | |
700 V Show Supplier Material materials with Kriechstromfestigkeit of 700 V | dry | Sim. to IEC 60112 | Above 600V | |
Surface resistivity | 3e+13 Ω/sq Show Supplier Material materials with Surface resistivity of 3e+13 Ω/sq | conditioned | IEC 62631-3-2 | |
1e+15 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+15 Ω/sq | dry | IEC 62631-3-2 | ||
Verlustfaktor | 100 [-] Show Supplier Material materials with Verlustfaktor of 100 [-] | dry | IEC 60250 | 1GHz |
110 [-] Show Supplier Material materials with Verlustfaktor of 110 [-] | dry, conditioned | IEC 62631-2-1 | 100Hz | |
140 [-] Show Supplier Material materials with Verlustfaktor of 140 [-] | conditioned | IEC 60250 | 1GHz | |
150 [-] Show Supplier Material materials with Verlustfaktor of 150 [-] | dry | IEC 62631-2-1 | 1MHz | |
490 [-] Show Supplier Material materials with Verlustfaktor of 490 [-] | conditioned | IEC 62631-2-1 | 1MHz | |
Volume resistivity | 5e+12 Ω·cm Show Supplier Material materials with Volume resistivity of 5e+12 Ω·cm | conditioned | IEC 62631-3-1 | |
1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 62631-3-1 |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Schrumpfung | 0.28 % Show Supplier Material materials with Schrumpfung of 0.28 % | dry | ISO 294-4 | Parallel |
1.31 % Show Supplier Material materials with Schrumpfung of 1.31 % | dry | ISO 294-4 | Normal | |
Spiral flow length | 87 | dry | - | 1.0 mm 800 bar |
104 | dry | - | 1.0 mm 1000 bar | |
121 | dry | - | 1.0 mm 1200 bar |
Technological properties
Property | ||
---|---|---|
Application areas | High voltage connector e-motor, High voltage connector, EV Charging Plugs | |
Certifications | Yellow Card Available | |
Fillers | 30% Glass Fiber |