Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 1.25 g/cm³ Show Supplier Material materials with Dichte of 1.25 g/cm³ | dry | ISO 1183 |
Wasserabsorption | 33 % Show Supplier Material materials with Wasserabsorption of 33 % | dry | Sim. to ISO 62 |
Mechanisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Dehnung | 280 % Show Supplier Material materials with Dehnung of 280 % | dry | ISO 527-1/-2 | |
Elastizitätsmodul | 0.11 GPa Show Supplier Material materials with Elastizitätsmodul of 0.11 GPa | dry | ISO 527-1/-2 | |
Härte, Shore D | 45 [-] Show Supplier Material materials with Härte, Shore D of 45 [-] | dry | ISO 868 | 3s |
Zugfestigkeit | 20 MPa Show Supplier Material materials with Zugfestigkeit of 20 MPa | dry | ISO 527-1/-2 |
Thermisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Schmelzpunkt | 185 °C Show Supplier Material materials with Schmelzpunkt of 185 °C | dry | ISO 11357-1/-3 | 10°C/min |
Vicat-Erweichungstemperatur | 44 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 44 °C | dry | ISO 306 | 50°C/h 50N |
156 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 156 °C | dry | ISO 306 | 50°C/h 10N |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Schmelzvolumenflussrate | 230 °C | 10 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 10 cm³/10min | dry | ISO 1133 |
Technological properties
Property | ||
---|---|---|
Application areas | Roofing membranes, Breathable Outdoor clothing, Breathable Films for Food Packaging, Smokable Sausage Casings | |
Certifications | Food Contact, USP class VI |