Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 1.56 g/cm³ Show Supplier Material materials with Dichte of 1.56 g/cm³ | dry | ISO 1183 |
Moisture absorption | 0.15 % Show Supplier Material materials with Moisture absorption of 0.15 % | dry | Sim. to ISO 62 |
Wasserabsorption | 0.3 % Show Supplier Material materials with Wasserabsorption of 0.3 % | dry | Sim. to ISO 62 |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Biegemodul | 6.6 GPa Show Supplier Material materials with Biegemodul of 6.6 GPa | dry | ISO 178 | |
120 °C | 2.7 GPa Show Supplier Material materials with Biegemodul of 2.7 GPa | dry | ISO 178 | |
160 °C | 1.9 GPa Show Supplier Material materials with Biegemodul of 1.9 GPa | dry | ISO 178 | |
Dehnung | -40 °C | 2.5 % Show Supplier Material materials with Dehnung of 2.5 % | dry | ISO 527-1/-2 |
2.9 % Show Supplier Material materials with Dehnung of 2.9 % | dry | ISO 527-1/-2 | ||
120 °C | 5.5 % Show Supplier Material materials with Dehnung of 5.5 % | dry | ISO 527-1/-2 | |
160 °C | 7 % Show Supplier Material materials with Dehnung of 7 % | dry | ISO 527-1/-2 | |
180 °C | 8 % Show Supplier Material materials with Dehnung of 8 % | dry | ISO 527-1/-2 | |
Elastizitätsmodul | -40 °C | 7.6 GPa Show Supplier Material materials with Elastizitätsmodul of 7.6 GPa | dry | ISO 527-1/-2 |
7 GPa Show Supplier Material materials with Elastizitätsmodul of 7 GPa | dry | ISO 527-1/-2 | ||
100 °C | 3.1 GPa Show Supplier Material materials with Elastizitätsmodul of 3.1 GPa | dry | ISO 527-1/-2 | |
120 °C | 2.7 GPa Show Supplier Material materials with Elastizitätsmodul of 2.7 GPa | dry | ISO 527-1/-2 | |
160 °C | 1.8 GPa Show Supplier Material materials with Elastizitätsmodul of 1.8 GPa | dry | ISO 527-1/-2 | |
180 °C | 1.4 GPa Show Supplier Material materials with Elastizitätsmodul of 1.4 GPa | dry | ISO 527-1/-2 | |
Flexural yield strength | 160 MPa Show Supplier Material materials with Flexural yield strength of 160 MPa | dry | ISO 178 | |
120 °C | 70 MPa Show Supplier Material materials with Flexural yield strength of 70 MPa | dry | ISO 178 | |
160 °C | 45 MPa Show Supplier Material materials with Flexural yield strength of 45 MPa | dry | ISO 178 | |
Schlagfestigkeit, Charpy gekerbt | -30 °C | 6 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 6 kJ/m² | dry | ISO 179/1eA |
23 °C | 6 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 6 kJ/m² | dry | ISO 179/1eA | |
Schlagzähigkeit, Charpy ungekerbt | -30 °C | 25 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 25 kJ/m² | dry | ISO 179/1eU |
23 °C | 35 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 35 kJ/m² | dry | ISO 179/1eU | |
Zugfestigkeit | -40 °C | 133 MPa Show Supplier Material materials with Zugfestigkeit of 133 MPa | dry | ISO 527-1/-2 |
105 MPa Show Supplier Material materials with Zugfestigkeit of 105 MPa | dry | ISO 527-1/-2 | ||
100 °C | 55.0 MPa Show Supplier Material materials with Zugfestigkeit of 55.0 MPa | dry | ISO 527-1/-2 | |
120 °C | 50 MPa Show Supplier Material materials with Zugfestigkeit of 50 MPa | dry | ISO 527-1/-2 | |
160 °C | 40 MPa Show Supplier Material materials with Zugfestigkeit of 40 MPa | dry | ISO 527-1/-2 | |
180 °C | 35 MPa Show Supplier Material materials with Zugfestigkeit of 35 MPa | dry | ISO 527-1/-2 |
Thermisch
Property | Value | Condition | Thickness | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|---|
Entflammbarkeit | V-0 | dry | 1.5 mm | IEC 60695-11-10 | UL recognition :Yes | |
5VB | dry | 1.5 mm | IEC 60695-11-20 | |||
Glow Wire Flammability Index | 960 °C Show Supplier Material materials with Glow Wire Flammability Index of 960 °C | dry | 2 mm | IEC 60695-2-12 | ||
960 °C Show Supplier Material materials with Glow Wire Flammability Index of 960 °C | dry | 0.75 mm | IEC 60695-2-12 | |||
Glow Wire Ignition Temperature | 725 °C Show Supplier Material materials with Glow Wire Ignition Temperature of 725 °C | dry | 2 mm | IEC 60695-2-13 | ||
800 °C Show Supplier Material materials with Glow Wire Ignition Temperature of 800 °C | dry | 0.75 mm | IEC 60695-2-13 | |||
Koeffizient der thermischen Ausdehnung | 5e-07 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 5e-07 1/K | dry | ISO 11359-1/-2 | Parallel | ||
8e-07 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 8e-07 1/K | dry | ISO 11359-1/-2 | Normal | |||
Relative temperature index, electrical | 130 °C Show Supplier Material materials with Relative temperature index, electrical of 130 °C | dry | 0.75 mm | UL746B | ||
Relative temperature index, mechanical impact | 140 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 140 °C | dry | 0.75 mm | UL746B | ||
Relative temperature index, mechanical strength | 130 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 130 °C | dry | 0.75 mm | UL746B | ||
Schmelzpunkt | 225 °C Show Supplier Material materials with Schmelzpunkt of 225 °C | dry | ISO 11357-1/-3 | 10°C/min | ||
Wärmeformbeständigkeitstemperatur | 200 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 200 °C | dry | ISO 75-1/-2 | 2 MPa | ||
215 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 215 °C | dry | ISO 75-1/-2 | 0.45 MPa |
Elektrisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Dielektrizitätskonstante | 3.5 [-] Show Supplier Material materials with Dielektrizitätskonstante of 3.5 [-] | dry | IEC 62631-2-1 | 1MHz |
3.7 [-] Show Supplier Material materials with Dielektrizitätskonstante of 3.7 [-] | dry | IEC 62631-2-1 | 100Hz | |
Durchschlagfestigkeit | 28.0 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 28.0 kV/mm | dry | IEC 60243-1 | |
Kriechstromfestigkeit | 250 V Show Supplier Material materials with Kriechstromfestigkeit of 250 V | dry | IEC 60112 | |
Verlustfaktor | 25 [-] Show Supplier Material materials with Verlustfaktor of 25 [-] | dry | IEC 62631-2-1 | 100Hz |
140 [-] Show Supplier Material materials with Verlustfaktor of 140 [-] | dry | IEC 62631-2-1 | 1MHz | |
Volume resistivity | 1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 62631-3-1 |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Schmelzmassenflussrate | 250 °C | 9 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 9 g/10min | dry | ISO 1133 | |
Schmelzvolumenflussrate | 250 °C | 7 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 7 cm³/10min | dry | ISO 1133 | |
Schrumpfung | 0.9 % Show Supplier Material materials with Schrumpfung of 0.9 % | dry | ISO 294-4 | Parallel | |
1.2 % Show Supplier Material materials with Schrumpfung of 1.2 % | dry | ISO 294-4 | Normal |
Technological properties
Property | ||
---|---|---|
Certifications | Yellow Card Available | |
Fillers | 15% Glass Fiber |