Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 1.34 g/cm³ Show Supplier Material materials with Dichte of 1.34 g/cm³ | dry | ISO 1183 |
Moisture absorption | 0.5 % Show Supplier Material materials with Moisture absorption of 0.5 % | dry | Sim. to ISO 62 |
Wasserabsorption | 0.9 % Show Supplier Material materials with Wasserabsorption of 0.9 % | dry | Sim. to ISO 62 |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Biegemodul | 2.5 GPa Show Supplier Material materials with Biegemodul of 2.5 GPa | dry | ISO 178 | |
Dehnung | 50 % Show Supplier Material materials with Dehnung of 50 % | dry | ISO 527-1/-2 | |
Elastizitätsmodul | 2.4 GPa Show Supplier Material materials with Elastizitätsmodul of 2.4 GPa | dry | ISO 527-1/-2 | |
Elongation at yield | 4 % Show Supplier Material materials with Elongation at yield of 4 % | dry | ISO 527-1/-2 | |
Flexural yield strength | 80 MPa Show Supplier Material materials with Flexural yield strength of 80 MPa | dry | ISO 178 | |
Schlagfestigkeit, Charpy gekerbt | -30 °C | 1.5 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 1.5 kJ/m² | dry | ISO 179/1eA |
23 °C | 2.9 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 2.9 kJ/m² | dry | ISO 179/1eA | |
Zugfestigkeit | 27 MPa Show Supplier Material materials with Zugfestigkeit of 27 MPa | dry | ISO 527-1/-2 |
Thermisch
Property | Value | Condition | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|
Schmelzpunkt | 255 °C Show Supplier Material materials with Schmelzpunkt of 255 °C | dry | ISO 11357-1/-3 | 10°C/min | |
Wärmeformbeständigkeitstemperatur | 65 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 65 °C | dry | ISO 75-1/-2 | 2 MPa | |
71 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 71 °C | dry | ISO 75-1/-2 | 0.45 MPa |
Elektrisch
Property | Value | Condition | Testing Standard |
---|---|---|---|
Volume resistivity | 1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 62631-3-1 |
Technological properties
Property |
---|