Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 1.59 g/cm³ Show Supplier Material materials with Dichte of 1.59 g/cm³ | dry | ISO 1183 |
Moisture absorption | 0.15 % Show Supplier Material materials with Moisture absorption of 0.15 % | dry | Sim. to ISO 62 |
Wasserabsorption | 0.3 % Show Supplier Material materials with Wasserabsorption of 0.3 % | dry | Sim. to ISO 62 |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Biegemodul | 7.5 GPa Show Supplier Material materials with Biegemodul of 7.5 GPa | dry | ISO 178 | |
Dehnung | 2.4 % Show Supplier Material materials with Dehnung of 2.4 % | dry | ISO 527-1/-2 | |
Elastizitätsmodul | 8 GPa Show Supplier Material materials with Elastizitätsmodul of 8 GPa | dry | ISO 527-1/-2 | |
Flexural yield strength | 150 MPa Show Supplier Material materials with Flexural yield strength of 150 MPa | dry | ISO 178 | |
Schlagfestigkeit, Charpy gekerbt | -30 °C | 6 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 6 kJ/m² | dry | ISO 179/1eA |
23 °C | 6 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 6 kJ/m² | dry | ISO 179/1eA | |
Schlagzähigkeit, Charpy ungekerbt | -30 °C | 40 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 40 kJ/m² | dry | ISO 179/1eU |
23 °C | 40 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 40 kJ/m² | dry | ISO 179/1eU | |
Zugfestigkeit | 105 MPa Show Supplier Material materials with Zugfestigkeit of 105 MPa | dry | ISO 527-1/-2 |
Thermisch
Property | Value | Condition | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|
Koeffizient der thermischen Ausdehnung | 4e-07 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 4e-07 1/K | dry | ISO 11359-1/-2 | Parallel | |
8e-07 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 8e-07 1/K | dry | ISO 11359-1/-2 | Normal | ||
Schmelzpunkt | 225 °C Show Supplier Material materials with Schmelzpunkt of 225 °C | dry | ISO 11357-1/-3 | 10°C/min | |
Wärmeformbeständigkeitstemperatur | 210 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 210 °C | dry | ISO 75-1/-2 | 2 MPa | |
220 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 220 °C | dry | ISO 75-1/-2 | 0.45 MPa |
Elektrisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Dielektrizitätskonstante | 3.7 [-] Show Supplier Material materials with Dielektrizitätskonstante of 3.7 [-] | dry | IEC 62631-2-1 | 1MHz |
3.9 [-] Show Supplier Material materials with Dielektrizitätskonstante of 3.9 [-] | dry | IEC 62631-2-1 | 100Hz | |
Durchschlagfestigkeit | 27 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 27 kV/mm | dry | IEC 60243-1 | |
Kriechstromfestigkeit | 250 V Show Supplier Material materials with Kriechstromfestigkeit of 250 V | dry | IEC 60112 | |
Verlustfaktor | 20 [-] Show Supplier Material materials with Verlustfaktor of 20 [-] | dry | IEC 62631-2-1 | 100Hz |
150 [-] Show Supplier Material materials with Verlustfaktor of 150 [-] | dry | IEC 62631-2-1 | 1MHz | |
Volume resistivity | 1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 62631-3-1 |
Technological properties
Property | ||
---|---|---|
Fillers | 20% Glass Fiber |