EcoPaXX® Q-HXG10 (Q-X07970)

Alternative und Handelsbezeichungen
PA410-GF50
Want to keep this datasheet? Save it now in your required format

Description

EcoPaXX® is our bio-based, high-performance polyamide (PA410) that offers outstanding performance across the board, while being made mainly from tropical castor beans which don’t compete with the food chain.
EcoPaXX® belongs to the family of long-chain polyamides, which offer exceptional performance in the most demanding of environments. That includes excellent chemical resistance, low moisture absorption, combined with a very high melting point (highest of all bio-plastics) and high crystallization rate (typical for engineering plastics like PA66 and PA46).
EcoPaXX® has the lowest carbon footprint amongst common polyamides. This is because the amount of carbon dioxide emitted during the production of EcoPaXX® is offset by the amount absorbed in plant growth, and in particular by the riccinus communis – the tropical castor bean plant that makes up some 70% of EcoPaXX®. Externally certified lifecycle analysis (LCA) data is available upon request.

Datasheet URL:

EcoPaXX® Q-HXG10 (Q-X07970)

Diese Materialdaten wurden von DSM zur Verfügung gestellt

Alle Daten beziehen sich auf Raumtemperatur soweit nicht anderweitig spezifiziert. SI Einheiten werden verwendt soweit nicht anderweitig spezifiziert.
Äquivalente Standards sind ähnlich zu einem oder mehreren Standards die der Anbieter angegeben hat. Manche äquivalente Standards können strikter sein oder außerhalb der Bedingungen des ursprünglichen Standards.

Ashby charts

Eigenschaften

Allgemein

PropertyValueConditionTesting Standard

Moisture absorption

1.2 %

Show Supplier Material materials with Moisture absorption of 1.2 %

dry

Sim. to ISO 62

Mechanisch

PropertyTemperatureValueConditionTesting Standard

Dehnung

3 %

Show Supplier Material materials with Dehnung of 3 %

dry

ISO 527-1/-2

6 %

Show Supplier Material materials with Dehnung of 6 %

conditioned

ISO 527-1/-2

80 °C

7 %

Show Supplier Material materials with Dehnung of 7 %

dry

ISO 527-1/-2

120 °C

8 %

Show Supplier Material materials with Dehnung of 8 %

dry

ISO 527-1/-2

140 °C

8.5 %

Show Supplier Material materials with Dehnung of 8.5 %

dry

ISO 527-1/-2

160 °C

9.3 %

Show Supplier Material materials with Dehnung of 9.3 %

dry

ISO 527-1/-2

180 °C

11 %

Show Supplier Material materials with Dehnung of 11 %

dry

ISO 527-1/-2

200 °C

12 %

Show Supplier Material materials with Dehnung of 12 %

dry

ISO 527-1/-2

Elastizitätsmodul

11 GPa

Show Supplier Material materials with Elastizitätsmodul of 11 GPa

conditioned

ISO 527-1/-2

16 GPa

Show Supplier Material materials with Elastizitätsmodul of 16 GPa

dry

ISO 527-1/-2

80 °C

8 GPa

Show Supplier Material materials with Elastizitätsmodul of 8 GPa

dry

ISO 527-1/-2

120 °C

7 GPa

Show Supplier Material materials with Elastizitätsmodul of 7 GPa

dry

ISO 527-1/-2

140 °C

6.2 GPa

Show Supplier Material materials with Elastizitätsmodul of 6.2 GPa

dry

ISO 527-1/-2

160 °C

5.7 GPa

Show Supplier Material materials with Elastizitätsmodul of 5.7 GPa

dry

ISO 527-1/-2

180 °C

5 GPa

Show Supplier Material materials with Elastizitätsmodul of 5 GPa

dry

ISO 527-1/-2

200 °C

4.5 GPa

Show Supplier Material materials with Elastizitätsmodul of 4.5 GPa

dry

ISO 527-1/-2

Schlagfestigkeit, Charpy gekerbt

-30 °C

11 kJ/m²

Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 11 kJ/m²

dry

ISO 179/1eA

23 °C

14.0 kJ/m²

Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 14.0 kJ/m²

dry

ISO 179/1eA

23 °C

18 kJ/m²

Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 18 kJ/m²

conditioned

ISO 179/1eA

Schlagzähigkeit, Charpy ungekerbt

-30 °C

92 kJ/m²

Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 92 kJ/m²

dry

ISO 179/1eU

23 °C

90 kJ/m²

Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 90 kJ/m²

dry

ISO 179/1eU

23 °C

98 kJ/m²

Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 98 kJ/m²

conditioned

ISO 179/1eU

Zugfestigkeit

150 MPa

Show Supplier Material materials with Zugfestigkeit of 150 MPa

conditioned

ISO 527-1/-2

220 MPa

Show Supplier Material materials with Zugfestigkeit of 220 MPa

dry

ISO 527-1/-2

80 °C

130 MPa

Show Supplier Material materials with Zugfestigkeit of 130 MPa

dry

ISO 527-1/-2

120 °C

115 MPa

Show Supplier Material materials with Zugfestigkeit of 115 MPa

dry

ISO 527-1/-2

140 °C

100 MPa

Show Supplier Material materials with Zugfestigkeit of 100 MPa

dry

ISO 527-1/-2

160 °C

90 MPa

Show Supplier Material materials with Zugfestigkeit of 90 MPa

dry

ISO 527-1/-2

180 °C

85 MPa

Show Supplier Material materials with Zugfestigkeit of 85 MPa

dry

ISO 527-1/-2

200 °C

70 MPa

Show Supplier Material materials with Zugfestigkeit of 70 MPa

dry

ISO 527-1/-2

Thermisch

PropertyValueConditionTesting StandardComment

Schmelzpunkt

250 °C

Show Supplier Material materials with Schmelzpunkt of 250 °C

dry

ISO 11357-1/-3

10°C/min

Technological properties

Property
Fillers

50% Glass Fiber