Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 1.12 g/cm³ Show Supplier Material materials with Dichte of 1.12 g/cm³ | dry | ISO 1183 |
Moisture absorption | 2.5 % Show Supplier Material materials with Moisture absorption of 2.5 % | dry | Sim. to ISO 62 |
Wasserabsorption | 9 % Show Supplier Material materials with Wasserabsorption of 9 % | dry | Sim. to ISO 62 |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Biegemodul | 2.9 GPa Show Supplier Material materials with Biegemodul of 2.9 GPa | dry | ISO 178 | |
Dehnung | 14.0 % Show Supplier Material materials with Dehnung of 14.0 % | dry | ISO 527-1/-2 | |
Elastizitätsmodul | 3.5 GPa Show Supplier Material materials with Elastizitätsmodul of 3.5 GPa | dry | ISO 527-1/-2 | |
Elongation at yield | 3.5 % Show Supplier Material materials with Elongation at yield of 3.5 % | dry | ISO 527-1/-2 | |
Flexural yield strength | 110 MPa Show Supplier Material materials with Flexural yield strength of 110 MPa | dry | ISO 178 | |
Schlagfestigkeit, Charpy gekerbt | 23 °C | 4 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 4 kJ/m² | dry | ISO 179/1eA |
Thermisch
Technological properties
Property |
---|