Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 1.13 g/cm³ Show Supplier Material materials with Dichte of 1.13 g/cm³ | dry | ISO 1183 |
Moisture absorption | 2.8 % Show Supplier Material materials with Moisture absorption of 2.8 % | dry | Sim. to ISO 62 |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Biegemodul | 2.8 GPa Show Supplier Material materials with Biegemodul of 2.8 GPa | dry | ISO 178 | |
Dehnung | 18 % Show Supplier Material materials with Dehnung of 18 % | dry | ISO 527-1/-2 | |
Elastizitätsmodul | 3.3 GPa Show Supplier Material materials with Elastizitätsmodul of 3.3 GPa | dry | ISO 527-1/-2 | |
Flexural yield strength | 114 MPa Show Supplier Material materials with Flexural yield strength of 114 MPa | dry | ISO 178 | |
Schlagfestigkeit, Charpy gekerbt | 23 °C | 4.1 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 4.1 kJ/m² | dry | ISO 179/1eA |
Thermisch
Property | Value | Condition | Thickness | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|---|
Entflammbarkeit | V-2 | dry | 1.5 mm | IEC 60695-11-10 | UL recognition :Yes | |
Relative temperature index, electrical | 130 °C Show Supplier Material materials with Relative temperature index, electrical of 130 °C | dry | 0.81 mm | UL746B | ||
Relative temperature index, mechanical impact | 65 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 65 °C | dry | 0.81 mm | UL746B | ||
Relative temperature index, mechanical strength | 80 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 80 °C | dry | 0.81 mm | UL746B | ||
Schmelzpunkt | 220 °C Show Supplier Material materials with Schmelzpunkt of 220 °C | dry | ISO 11357-1/-3 | 10°C/min | ||
Wärmeformbeständigkeitstemperatur | 76 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 76 °C | dry | ISO 75-1/-2 | 2 MPa | ||
173 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 173 °C | dry | ISO 75-1/-2 | 0.45 MPa |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Schmelzmassenflussrate | 230 °C | 50 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 50 g/10min | dry | ISO 1133 | |
Schmelzvolumenflussrate | 230 °C | 44 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 44 cm³/10min | dry | ISO 1133 | |
Schrumpfung | 1.1 % Show Supplier Material materials with Schrumpfung of 1.1 % | dry | Sim. to ISO 294-4 | Parallel | |
1.3 % Show Supplier Material materials with Schrumpfung of 1.3 % | dry | Sim. to ISO 294-4 | Normal | ||
Viscosity number | 118 cm³/gr Show Supplier Material materials with Viscosity number of 118 cm³/gr | dry | ISO 307, 1157, 1628 |
Technological properties
Property | ||
---|---|---|
Certifications | Yellow Card Available |