Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 1.23 g/cm³ Show Supplier Material materials with Dichte of 1.23 g/cm³ | dry | ISO 1183 |
Moisture absorption | 2.3 % Show Supplier Material materials with Moisture absorption of 2.3 % | dry | Sim. to ISO 62 |
Wasserabsorption | 7.6 % Show Supplier Material materials with Wasserabsorption of 7.6 % | dry | Sim. to ISO 62 |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Biegemodul | 5.2 GPa Show Supplier Material materials with Biegemodul of 5.2 GPa | dry | ISO 178 | |
Dehnung | 3 % Show Supplier Material materials with Dehnung of 3 % | dry | ISO 527-1/-2 | |
12 % Show Supplier Material materials with Dehnung of 12 % | conditioned | ISO 527-1/-2 | ||
Elastizitätsmodul | 3.5 GPa Show Supplier Material materials with Elastizitätsmodul of 3.5 GPa | conditioned | ISO 527-1/-2 | |
6 GPa Show Supplier Material materials with Elastizitätsmodul of 6 GPa | dry | ISO 527-1/-2 | ||
Flexural yield strength | 170 MPa Show Supplier Material materials with Flexural yield strength of 170 MPa | dry | ISO 178 | |
Schlagfestigkeit, Charpy gekerbt | -30 °C | 6 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 6 kJ/m² | dry, conditioned | ISO 179/1eA |
23 °C | 7 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 7 kJ/m² | dry | ISO 179/1eA | |
23 °C | 15 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 15 kJ/m² | conditioned | ISO 179/1eA | |
Schlagzähigkeit, Charpy ungekerbt | -30 °C | 40 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 40 kJ/m² | dry, conditioned | ISO 179/1eU |
23 °C | 45 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 45 kJ/m² | dry | ISO 179/1eU | |
23 °C | 80 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 80 kJ/m² | conditioned | ISO 179/1eU | |
Zugfestigkeit | 70 MPa Show Supplier Material materials with Zugfestigkeit of 70 MPa | conditioned | ISO 527-1/-2 | |
125 MPa Show Supplier Material materials with Zugfestigkeit of 125 MPa | dry | ISO 527-1/-2 |
Thermisch
Property | Value | Condition | Thickness | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|---|
Entflammbarkeit | HB | dry | 1.5 mm | IEC 60695-11-10 | UL recognition :Yes | |
Koeffizient der thermischen Ausdehnung | 3e-07 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 3e-07 1/K | dry | ISO 11359-1/-2 | Parallel | ||
8e-07 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 8e-07 1/K | dry | ISO 11359-1/-2 | Normal | |||
Relative temperature index, electrical | 150 °C Show Supplier Material materials with Relative temperature index, electrical of 150 °C | dry | 0.71 mm | UL746B | ||
Relative temperature index, mechanical impact | 120 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 120 °C | dry | 0.71 mm | UL746B | ||
Relative temperature index, mechanical strength | 150 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 150 °C | dry | 0.71 mm | UL746B | ||
Schmelzpunkt | 220 °C Show Supplier Material materials with Schmelzpunkt of 220 °C | dry | ISO 11357-1/-3 | 10°C/min | ||
Temperaturleitfähigkeit | 1.03e-07 mm²/s Show Supplier Material materials with Temperaturleitfähigkeit of 1.03e-07 mm²/s | dry | - | |||
Wärmeformbeständigkeitstemperatur | 195 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 195 °C | dry | ISO 75-1/-2 | 2 MPa | ||
215 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 215 °C | dry | ISO 75-1/-2 | 0.45 MPa |
Elektrisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Dielektrizitätskonstante | 4 [-] Show Supplier Material materials with Dielektrizitätskonstante of 4 [-] | dry | IEC 62631-2-1 | 1MHz |
4.6 [-] Show Supplier Material materials with Dielektrizitätskonstante of 4.6 [-] | dry | IEC 62631-2-1 | 100Hz | |
Durchschlagfestigkeit | 20 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 20 kV/mm | conditioned | IEC 60243-1 | |
25 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 25 kV/mm | dry | IEC 60243-1 | ||
Kriechstromfestigkeit | 425 V Show Supplier Material materials with Kriechstromfestigkeit of 425 V | conditioned | IEC 60112 | |
Surface resistivity | 1e+13 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+13 Ω/sq | conditioned | IEC 62631-3-2 | |
Verlustfaktor | 230 [-] Show Supplier Material materials with Verlustfaktor of 230 [-] | dry | IEC 62631-2-1 | 100Hz |
270 [-] Show Supplier Material materials with Verlustfaktor of 270 [-] | dry | IEC 62631-2-1 | 1MHz | |
Volume resistivity | 1e+10 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+10 Ω·cm | conditioned | IEC 62631-3-1 | |
1e+12 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+12 Ω·cm | dry | IEC 62631-3-1 |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Density of melt | 1030 g/cm³ Show Supplier Material materials with Density of melt of 1030 g/cm³ | dry | - | |
Schrumpfung | 0.25 % Show Supplier Material materials with Schrumpfung of 0.25 % | dry | ISO 294-4 | Parallel |
1.1 % Show Supplier Material materials with Schrumpfung of 1.1 % | dry | ISO 294-4 | Normal | |
Specific heat capacity melt | 2400 J/(kg·K) Show Supplier Material materials with Specific heat capacity melt of 2400 J/(kg·K) | dry | - | |
Thermal conductivity of melt | 0.26 W/(m·K) Show Supplier Material materials with Thermal conductivity of melt of 0.26 W/(m·K) | dry | - |
Technological properties
Property | ||
---|---|---|
Certifications | Yellow Card Available | |
Fillers | 15% Glass Fiber |