Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 1.15 g/cm³ Show Supplier Material materials with Dichte of 1.15 g/cm³ | dry | ISO 1183 |
Moisture absorption | 0.3 % Show Supplier Material materials with Moisture absorption of 0.3 % | dry | Sim. to ISO 62 |
Wasserabsorption | 0.7 % Show Supplier Material materials with Wasserabsorption of 0.7 % | dry | Sim. to ISO 62 |
Mechanisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Dehnung | 50 % Show Supplier Material materials with Dehnung of 50 % | dry | ISO 527-1/-2 | |
300 % Show Supplier Material materials with Dehnung of 300 % | dry | ISO 527-1/-2 | ||
Elastizitätsmodul | 0.09 GPa Show Supplier Material materials with Elastizitätsmodul of 0.09 GPa | dry | ISO 527-1/-2 | |
Elongation at yield | 45 % Show Supplier Material materials with Elongation at yield of 45 % | dry | ISO 527-1/-2 | |
Härte, Shore D | 40 [-] Show Supplier Material materials with Härte, Shore D of 40 [-] | dry | ISO 868 | 3s |
Reißfestigkeit | 100 kN/m Show Supplier Material materials with Reißfestigkeit of 100 kN/m | dry | ISO 34-1; Method B | |
Zugfestigkeit | 23 MPa Show Supplier Material materials with Zugfestigkeit of 23 MPa | dry | ISO 527-1/-2 |
Thermisch
Property | Value | Condition | Thickness | Testing Standard | Comment |
---|---|---|---|---|---|
Entflammbarkeit | HB | dry | 1.5 mm | IEC 60695-11-10 | UL recognition :Yes |
Koeffizient der thermischen Ausdehnung | 1.6e-06 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.6e-06 1/K | dry | ISO 11359-1/-2 | Parallel | |
1.6e-06 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.6e-06 1/K | dry | ISO 11359-1/-2 | Normal | ||
Relative temperature index, electrical | 50 °C Show Supplier Material materials with Relative temperature index, electrical of 50 °C | dry | 2 mm | UL746B | |
Relative temperature index, mechanical impact | 50 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 50 °C | dry | 2 mm | UL746B | |
Relative temperature index, mechanical strength | 50 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 50 °C | dry | 2 mm | UL746B | |
Schmelzpunkt | 189 °C Show Supplier Material materials with Schmelzpunkt of 189 °C | dry | ISO 11357-1/-3 | 10°C/min | |
Temperaturleitfähigkeit | 5.99e-08 mm²/s Show Supplier Material materials with Temperaturleitfähigkeit of 5.99e-08 mm²/s | dry | - | ||
Vicat-Erweichungstemperatur | 50 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 50 °C | dry | ISO 306 | 50°C/h 50N |
Elektrisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Dielektrizitätskonstante | 4.4 [-] Show Supplier Material materials with Dielektrizitätskonstante of 4.4 [-] | dry | IEC 62631-2-1 | 1MHz |
Durchschlagfestigkeit | 20 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 20 kV/mm | dry | IEC 60243-1 | |
Kriechstromfestigkeit | 600 V Show Supplier Material materials with Kriechstromfestigkeit of 600 V | dry | IEC 60112 | |
Verlustfaktor | 350 [-] Show Supplier Material materials with Verlustfaktor of 350 [-] | dry | IEC 62631-2-1 | 1MHz |
Volume resistivity | 1e+11 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+11 Ω·cm | dry | IEC 62631-3-1 |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Density of melt | 928 g/cm³ Show Supplier Material materials with Density of melt of 928 g/cm³ | dry | - | ||
Schmelzvolumenflussrate | 230 °C | 46 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 46 cm³/10min | dry | ISO 1133 | |
Schrumpfung | 1.25 % Show Supplier Material materials with Schrumpfung of 1.25 % | dry | Sim. to ISO 294-4 | Parallel | |
1.5 % Show Supplier Material materials with Schrumpfung of 1.5 % | dry | Sim. to ISO 294-4 | Normal | ||
Specific heat capacity melt | 1800 J/(kg·K) Show Supplier Material materials with Specific heat capacity melt of 1800 J/(kg·K) | dry | - | ||
Thermal conductivity of melt | 0.1 W/(m·K) Show Supplier Material materials with Thermal conductivity of melt of 0.1 W/(m·K) | dry | - |
Technological properties
Property | ||
---|---|---|
Application areas | Conveyor Belts, Spider Couplings, Virtual Reality, Optical Fiber Cable guides and connectors, Support Springs, Phone case | |
Certifications | Food Contact, Yellow Card Available |