Allgemein
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Dichte | 1.62 g/cm³ Show Supplier Material materials with Dichte of 1.62 g/cm³ | dry | ISO 1183 | |
Moisture absorption | 1.85 % Show Supplier Material materials with Moisture absorption of 1.85 % | dry | Sim. to ISO 62 | |
Sauerstoffindex | 22 % Show Supplier Material materials with Sauerstoffindex of 22 % | dry | ISO 4589-1/-2 | |
Wasserabsorption | 1.9 % Show Supplier Material materials with Wasserabsorption of 1.9 % | dry | ISO 62 | at 23°C after 24h |
6.75 % Show Supplier Material materials with Wasserabsorption of 6.75 % | dry | Sim. to ISO 62 |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Biegemodul | 9 GPa Show Supplier Material materials with Biegemodul of 9 GPa | conditioned | ISO 178 | |
15 GPa Show Supplier Material materials with Biegemodul of 15 GPa | dry | ISO 178 | ||
120 °C | 7.3 GPa Show Supplier Material materials with Biegemodul of 7.3 GPa | dry | ISO 178 | |
160 °C | 6.5 GPa Show Supplier Material materials with Biegemodul of 6.5 GPa | dry | ISO 178 | |
Dehnung | -40 °C | 2.3 % Show Supplier Material materials with Dehnung of 2.3 % | dry | ISO 527-1/-2 |
2.7 % Show Supplier Material materials with Dehnung of 2.7 % | dry | ISO 527-1/-2 | ||
5 % Show Supplier Material materials with Dehnung of 5 % | conditioned | ISO 527-1/-2 | ||
120 °C | 5 % Show Supplier Material materials with Dehnung of 5 % | dry | ISO 527-1/-2 | |
140 °C | 5 % Show Supplier Material materials with Dehnung of 5 % | dry | ISO 527-1/-2 | |
150 °C | 5.5 % Show Supplier Material materials with Dehnung of 5.5 % | dry | ISO 527-1/-2 | |
160 °C | 5.5 % Show Supplier Material materials with Dehnung of 5.5 % | dry | ISO 527-1/-2 | |
180 °C | 5.5 % Show Supplier Material materials with Dehnung of 5.5 % | dry | ISO 527-1/-2 | |
200 °C | 6 % Show Supplier Material materials with Dehnung of 6 % | dry | ISO 527-1/-2 | |
210 °C | 0.006 % Show Supplier Material materials with Dehnung of 0.006 % | dry | ISO 527-1/-2 | |
Elastizitätsmodul | -40 °C | 16.5 GPa Show Supplier Material materials with Elastizitätsmodul of 16.5 GPa | dry | ISO 527-1/-2 |
10 GPa Show Supplier Material materials with Elastizitätsmodul of 10 GPa | conditioned | ISO 527-1/-2 | ||
16 GPa Show Supplier Material materials with Elastizitätsmodul of 16 GPa | dry | ISO 527-1/-2 | ||
100 °C | 9.5 GPa Show Supplier Material materials with Elastizitätsmodul of 9.5 GPa | dry | ISO 527-1/-2 | |
120 °C | 8.5 GPa Show Supplier Material materials with Elastizitätsmodul of 8.5 GPa | dry | ISO 527-1/-2 | |
140 °C | 8 GPa Show Supplier Material materials with Elastizitätsmodul of 8 GPa | dry | ISO 527-1/-2 | |
150 °C | 7.6 GPa Show Supplier Material materials with Elastizitätsmodul of 7.6 GPa | dry | ISO 527-1/-2 | |
160 °C | 7.2 GPa Show Supplier Material materials with Elastizitätsmodul of 7.2 GPa | dry | ISO 527-1/-2 | |
180 °C | 6.6 GPa Show Supplier Material materials with Elastizitätsmodul of 6.6 GPa | dry | ISO 527-1/-2 | |
200 °C | 6 GPa Show Supplier Material materials with Elastizitätsmodul of 6 GPa | dry | ISO 527-1/-2 | |
210 °C | 5.8 GPa Show Supplier Material materials with Elastizitätsmodul of 5.8 GPa | dry | ISO 527-1/-2 | |
Flexural yield strength | 250 MPa Show Supplier Material materials with Flexural yield strength of 250 MPa | conditioned | ISO 178 | |
380 MPa Show Supplier Material materials with Flexural yield strength of 380 MPa | dry | ISO 178 | ||
120 °C | 180 MPa Show Supplier Material materials with Flexural yield strength of 180 MPa | dry | ISO 178 | |
160 °C | 150 MPa Show Supplier Material materials with Flexural yield strength of 150 MPa | dry | ISO 178 | |
Schlagfestigkeit, Charpy gekerbt | -30 °C | 14.0 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 14.0 kJ/m² | dry, conditioned | ISO 179/1eA |
23 °C | 16 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 16 kJ/m² | dry | ISO 179/1eA | |
23 °C | 24 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 24 kJ/m² | conditioned | ISO 179/1eA | |
Schlagzähigkeit, Charpy ungekerbt | -30 °C | 90 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 90 kJ/m² | dry | ISO 179/1eU |
-30 °C | 100 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 100 kJ/m² | conditioned | ISO 179/1eU | |
23 °C | 100 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 100 kJ/m² | dry | ISO 179/1eU | |
23 °C | 110 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 110 kJ/m² | conditioned | ISO 179/1eU | |
Zugfestigkeit | -40 °C | 290 MPa Show Supplier Material materials with Zugfestigkeit of 290 MPa | dry | ISO 527-1/-2 |
150 MPa Show Supplier Material materials with Zugfestigkeit of 150 MPa | conditioned | ISO 527-1/-2 | ||
250 MPa Show Supplier Material materials with Zugfestigkeit of 250 MPa | dry | ISO 527-1/-2 | ||
100 °C | 150 MPa Show Supplier Material materials with Zugfestigkeit of 150 MPa | dry | ISO 527-1/-2 | |
120 °C | 140 MPa Show Supplier Material materials with Zugfestigkeit of 140 MPa | dry | ISO 527-1/-2 | |
140 °C | 130 MPa Show Supplier Material materials with Zugfestigkeit of 130 MPa | dry | ISO 527-1/-2 | |
150 °C | 125 MPa Show Supplier Material materials with Zugfestigkeit of 125 MPa | dry | ISO 527-1/-2 | |
160 °C | 120 MPa Show Supplier Material materials with Zugfestigkeit of 120 MPa | dry | ISO 527-1/-2 | |
180 °C | 110 MPa Show Supplier Material materials with Zugfestigkeit of 110 MPa | dry | ISO 527-1/-2 | |
200 °C | 100 MPa Show Supplier Material materials with Zugfestigkeit of 100 MPa | dry | ISO 527-1/-2 | |
210 °C | 95 MPa Show Supplier Material materials with Zugfestigkeit of 95 MPa | dry | ISO 527-1/-2 |
Thermisch
Property | Value | Condition | Testing Standard | Thickness | Pressure | Comment |
---|---|---|---|---|---|---|
Glasübergangstemperatur | 75 °C Show Supplier Material materials with Glasübergangstemperatur of 75 °C | dry | ISO 11357-1/-2 | 10°C/min | ||
Koeffizient der thermischen Ausdehnung | 2.5e-07 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 2.5e-07 1/K | dry | ISO 11359-1/-2 | Parallel | ||
4e-07 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 4e-07 1/K | dry | ISO 11359-1/-2 | Normal | |||
Relative temperature index, electrical | 65 °C Show Supplier Material materials with Relative temperature index, electrical of 65 °C | dry | UL746B | 0.75 mm | ||
Relative temperature index, mechanical impact | 65 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 65 °C | dry | UL746B | 0.75 mm | ||
Relative temperature index, mechanical strength | 65 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 65 °C | dry | UL746B | 0.75 mm | ||
Schmelzpunkt | 295 °C Show Supplier Material materials with Schmelzpunkt of 295 °C | dry | ISO 11357-1/-3 | 10°C/min | ||
Temperaturleitfähigkeit | 1.39e-07 mm²/s Show Supplier Material materials with Temperaturleitfähigkeit of 1.39e-07 mm²/s | dry | - | |||
Vicat-Erweichungstemperatur | 290 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 290 °C | dry | ISO 306 | 50°C/h 50N | ||
Wärmeformbeständigkeitstemperatur | 290 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 290 °C | dry | ISO 75-1/-2 | 2 MPa | ||
290 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 290 °C | dry | ISO 75-1/-2 | 0.45 MPa |
Elektrisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Dielektrizitätskonstante | 4 [-] Show Supplier Material materials with Dielektrizitätskonstante of 4 [-] | dry | IEC 62631-2-1 | 1MHz |
4.3 [-] Show Supplier Material materials with Dielektrizitätskonstante of 4.3 [-] | dry | IEC 62631-2-1 | 100Hz | |
4.7 [-] Show Supplier Material materials with Dielektrizitätskonstante of 4.7 [-] | conditioned | IEC 62631-2-1 | 1MHz | |
16 [-] Show Supplier Material materials with Dielektrizitätskonstante of 16 [-] | conditioned | IEC 62631-2-1 | 100Hz | |
Durchschlagfestigkeit | 20 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 20 kV/mm | conditioned | IEC 60243-1 | |
30 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 30 kV/mm | dry | IEC 60243-1 | ||
Kriechstromfestigkeit | 300 V Show Supplier Material materials with Kriechstromfestigkeit of 300 V | dry | IEC 60112 | |
Surface resistivity | 1e+13 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+13 Ω/sq | conditioned | IEC 62631-3-2 | |
Verlustfaktor | 70 [-] Show Supplier Material materials with Verlustfaktor of 70 [-] | dry | IEC 62631-2-1 | 100Hz |
200 [-] Show Supplier Material materials with Verlustfaktor of 200 [-] | dry | IEC 62631-2-1 | 1MHz | |
1000 [-] Show Supplier Material materials with Verlustfaktor of 1000 [-] | conditioned | IEC 62631-2-1 | 1MHz | |
6000 [-] Show Supplier Material materials with Verlustfaktor of 6000 [-] | conditioned | IEC 62631-2-1 | 100Hz | |
Volume resistivity | 1e+08 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+08 Ω·cm | conditioned | IEC 62631-3-1 | |
1e+12 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+12 Ω·cm | dry | IEC 62631-3-1 |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Density of melt | 1420.0 g/cm³ Show Supplier Material materials with Density of melt of 1420.0 g/cm³ | dry | - | |
Schrumpfung | 0.4 % Show Supplier Material materials with Schrumpfung of 0.4 % | dry | Sim. to ISO 294-4 | Parallel |
0.9 % Show Supplier Material materials with Schrumpfung of 0.9 % | dry | Sim. to ISO 294-4 | Normal | |
Specific heat capacity melt | 1990 J/(kg·K) Show Supplier Material materials with Specific heat capacity melt of 1990 J/(kg·K) | dry | - | |
Spiral flow length | 70 | dry | - | 1.0 mm 800 bar |
80 | dry | - | 1.0 mm 900 bar | |
90 | dry | - | 1.0 mm 1000 bar | |
Thermal conductivity of melt | 0.391 W/(m·K) Show Supplier Material materials with Thermal conductivity of melt of 0.391 W/(m·K) | dry | - | |
Viscosity number | 140 cm³/gr Show Supplier Material materials with Viscosity number of 140 cm³/gr | dry | ISO 307, 1157, 1628 |
Technological properties
Property | ||
---|---|---|
Application areas | Off-road Vehicle Oil Pans and Reservoirs, MTF/DMF Components, Torque Convertor Components, Charge Air Cooler Caps, EPS Steering components: Gears, Flex couplers and Sensors, Wheel Speed Sensors, Endlaminates (electrical components), Gears, Timing drive systems, Electric parking brakes, Electric brake boosters, Electronic throttle control actuators, Exhaust gas recirculation actuators, Turbo actuators, Coolant valve actuators, Seat actuators, Mirror actuators, Trunk actuators, Door handle actuators, Sunroof actuators, Steering wheel adjusters | |
Certifications | Yellow Card Available | |
Fillers | 50% Glass Fiber |