Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 1.17 g/cm³ Show Supplier Material materials with Dichte of 1.17 g/cm³ | dry | ISO 1183 |
Mechanisch
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dehnung | 3 % Show Supplier Material materials with Dehnung of 3 % | dry | ISO 527-1/-2 |
Elastizitätsmodul | 7.6 GPa Show Supplier Material materials with Elastizitätsmodul of 7.6 GPa | dry | ISO 527-1/-2 |
Elongation at yield | 2.8 % Show Supplier Material materials with Elongation at yield of 2.8 % | dry | ISO 527-1/-2 |
Zugfestigkeit | 110 MPa Show Supplier Material materials with Zugfestigkeit of 110 MPa | dry | ISO 527-1/-2 |
Thermisch
Property | Value | Condition | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|
Glasübergangstemperatur | 58.0 °C Show Supplier Material materials with Glasübergangstemperatur of 58.0 °C | dry | ISO 11357-1/-2 | 10°C/min | |
Schmelzpunkt | 200 °C Show Supplier Material materials with Schmelzpunkt of 200 °C | dry | ISO 11357-1/-3 | 10°C/min | |
Wärmeformbeständigkeitstemperatur | 153 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 153 °C | dry | ISO 75-1/-2 | 2 MPa | |
184 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 184 °C | dry | ISO 75-1/-2 | 0.45 MPa |
Technological properties
Property | ||
---|---|---|
Fillers | 10% Carbon Fiber |