Akulon® is our family of high performance polyamide 6 and polyamide 66 materials, used by customers across the world in applications ranging from automotive, electronics & electrical, to furniture and packaging.
We offer Akulon® grades for injection molding, blow molding and extrusion (including barrier film, stock shapes, convoluted tubes, and mono and multi filament).
In molded parts the material offers an excellent balance of easy design and processing with outstanding mechanical properties over a wide temperature range and in diverse conditions. Meanwhile for extrusion the strength, resilience and easy processing of Akulon® sets the market standards.

Datasheet URL:

Akulon® S223-G6-FC NA99001

Diese Materialdaten wurden von DSM zur Verfügung gestellt

Alle Daten beziehen sich auf Raumtemperatur soweit nicht anderweitig spezifiziert. SI Einheiten werden verwendt soweit nicht anderweitig spezifiziert.
Äquivalente Standards sind ähnlich zu einem oder mehreren Standards die der Anbieter angegeben hat. Manche äquivalente Standards können strikter sein oder außerhalb der Bedingungen des ursprünglichen Standards.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Eigenschaften

Allgemein

PropertyValueConditionTesting Standard

Dichte

1.36 g/cm³

Show Supplier Material materials with Dichte of 1.36 g/cm³

dry

ISO 1183

Moisture absorption

1.6 %

Show Supplier Material materials with Moisture absorption of 1.6 %

dry

Sim. to ISO 62

Wasserabsorption

6 %

Show Supplier Material materials with Wasserabsorption of 6 %

dry

Sim. to ISO 62

Mechanisch

PropertyTemperatureValueConditionTesting Standard

Biegemodul

8.4 GPa

Show Supplier Material materials with Biegemodul of 8.4 GPa

dry

ISO 178

Dehnung

3 %

Show Supplier Material materials with Dehnung of 3 %

dry

ISO 527-1/-2

5 %

Show Supplier Material materials with Dehnung of 5 %

conditioned

ISO 527-1/-2

Elastizitätsmodul

7.5 GPa

Show Supplier Material materials with Elastizitätsmodul of 7.5 GPa

conditioned

ISO 527-1/-2

9.5 GPa

Show Supplier Material materials with Elastizitätsmodul of 9.5 GPa

dry

ISO 527-1/-2

Flexural yield strength

250 MPa

Show Supplier Material materials with Flexural yield strength of 250 MPa

dry

ISO 178

Schlagfestigkeit, Charpy gekerbt

-30 °C

10 kJ/m²

Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 10 kJ/m²

dry, conditioned

ISO 179/1eA

23 °C

12 kJ/m²

Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 12 kJ/m²

dry

ISO 179/1eA

23 °C

20 kJ/m²

Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 20 kJ/m²

conditioned

ISO 179/1eA

Schlagzähigkeit, Charpy ungekerbt

-30 °C

70 kJ/m²

Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 70 kJ/m²

dry, conditioned

ISO 179/1eU

23 °C

80 kJ/m²

Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 80 kJ/m²

dry

ISO 179/1eU

23 °C

100 kJ/m²

Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 100 kJ/m²

conditioned

ISO 179/1eU

Zugfestigkeit

140 MPa

Show Supplier Material materials with Zugfestigkeit of 140 MPa

conditioned

ISO 527-1/-2

190 MPa

Show Supplier Material materials with Zugfestigkeit of 190 MPa

dry

ISO 527-1/-2

Thermisch

PropertyValueConditionTesting StandardThicknessPressureComment

Koeffizient der thermischen Ausdehnung

2e-07 1/K

Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 2e-07 1/K

dry

ISO 11359-1/-2

Parallel

7e-07 1/K

Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 7e-07 1/K

dry

ISO 11359-1/-2

Normal

Relative temperature index, electrical

65 °C

Show Supplier Material materials with Relative temperature index, electrical of 65 °C

dry

UL746B

0.71 mm

Relative temperature index, mechanical impact

65 °C

Show Supplier Material materials with Relative temperature index, mechanical impact of 65 °C

dry

UL746B

0.71 mm

Relative temperature index, mechanical strength

65 °C

Show Supplier Material materials with Relative temperature index, mechanical strength of 65 °C

dry

UL746B

0.71 mm

Schmelzpunkt

260 °C

Show Supplier Material materials with Schmelzpunkt of 260 °C

dry

ISO 11357-1/-3

10°C/min

Wärmeformbeständigkeitstemperatur

245 °C

Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 245 °C

dry

ISO 75-1/-2

2 MPa

260 °C

Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 260 °C

dry

ISO 75-1/-2

0.45 MPa

Elektrisch

PropertyValueConditionTesting StandardComment

Dielektrizitätskonstante

3.5 [-]

Show Supplier Material materials with Dielektrizitätskonstante of 3.5 [-]

dry

IEC 62631-2-1

1MHz

3.8 [-]

Show Supplier Material materials with Dielektrizitätskonstante of 3.8 [-]

dry

IEC 62631-2-1

100Hz

4.6 [-]

Show Supplier Material materials with Dielektrizitätskonstante of 4.6 [-]

conditioned

IEC 62631-2-1

1MHz

11 [-]

Show Supplier Material materials with Dielektrizitätskonstante of 11 [-]

conditioned

IEC 62631-2-1

100Hz

Durchschlagfestigkeit

25 kV/mm

Show Supplier Material materials with Durchschlagfestigkeit of 25 kV/mm

conditioned

IEC 60243-1

30 kV/mm

Show Supplier Material materials with Durchschlagfestigkeit of 30 kV/mm

dry

IEC 60243-1

Kriechstromfestigkeit

600 V

Show Supplier Material materials with Kriechstromfestigkeit of 600 V

dry, conditioned

IEC 60112

Surface resistivity

1e+14 Ω/sq

Show Supplier Material materials with Surface resistivity of 1e+14 Ω/sq

conditioned

IEC 62631-3-2

Verlustfaktor

90 [-]

Show Supplier Material materials with Verlustfaktor of 90 [-]

dry

IEC 62631-2-1

100Hz

160 [-]

Show Supplier Material materials with Verlustfaktor of 160 [-]

dry

IEC 62631-2-1

1MHz

1000 [-]

Show Supplier Material materials with Verlustfaktor of 1000 [-]

conditioned

IEC 62631-2-1

1MHz

1400 [-]

Show Supplier Material materials with Verlustfaktor of 1400 [-]

conditioned

IEC 62631-2-1

100Hz

Volume resistivity

1e+11 Ω·cm

Show Supplier Material materials with Volume resistivity of 1e+11 Ω·cm

conditioned

IEC 62631-3-1

1e+13 Ω·cm

Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm

dry

IEC 62631-3-1

Rheological Properties

PropertyValueConditionTesting StandardComment

Schrumpfung

0.2 %

Show Supplier Material materials with Schrumpfung of 0.2 %

dry

Sim. to ISO 294-4

Parallel

1.2 %

Show Supplier Material materials with Schrumpfung of 1.2 %

dry

Sim. to ISO 294-4

Normal

Specific heat capacity melt

2170 J/(kg·K)

Show Supplier Material materials with Specific heat capacity melt of 2170 J/(kg·K)

dry

-

Thermal conductivity of melt

0.172 W/(m·K)

Show Supplier Material materials with Thermal conductivity of melt of 0.172 W/(m·K)

dry

-

Technological properties

Property
Application areas

Spatulas and Kitchenware

Certifications

Food Contact

Fillers

30% Glass Fiber