Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 1.44 g/cm³ Show Supplier Material materials with Dichte of 1.44 g/cm³ | dry | ISO 1183 |
Moisture absorption | 1.5 % Show Supplier Material materials with Moisture absorption of 1.5 % | dry | Sim. to ISO 62 |
Wasserabsorption | 5.6 % Show Supplier Material materials with Wasserabsorption of 5.6 % | dry | Sim. to ISO 62 |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Biegemodul | 3.7 GPa Show Supplier Material materials with Biegemodul of 3.7 GPa | conditioned | ISO 178 | |
7.5 GPa Show Supplier Material materials with Biegemodul of 7.5 GPa | dry | ISO 178 | ||
Dehnung | 3.2 % Show Supplier Material materials with Dehnung of 3.2 % | dry | ISO 527-1/-2 | |
20 % Show Supplier Material materials with Dehnung of 20 % | conditioned | ISO 527-1/-2 | ||
Elastizitätsmodul | 3.5 GPa Show Supplier Material materials with Elastizitätsmodul of 3.5 GPa | conditioned | ISO 527-1/-2 | |
7.8 GPa Show Supplier Material materials with Elastizitätsmodul of 7.8 GPa | dry | ISO 527-1/-2 | ||
Flexural yield strength | 80 MPa Show Supplier Material materials with Flexural yield strength of 80 MPa | conditioned | ISO 178 | |
160 MPa Show Supplier Material materials with Flexural yield strength of 160 MPa | dry | ISO 178 | ||
Schlagfestigkeit, Charpy gekerbt | -30 °C | 3 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 3 kJ/m² | dry, conditioned | ISO 179/1eA |
23 °C | 4 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 4 kJ/m² | dry | ISO 179/1eA | |
23 °C | 7 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 7 kJ/m² | conditioned | ISO 179/1eA | |
Schlagzähigkeit, Charpy ungekerbt | -30 °C | 40 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 40 kJ/m² | dry, conditioned | ISO 179/1eU |
23 °C | 43 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 43 kJ/m² | dry | ISO 179/1eU | |
23 °C | 80 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 80 kJ/m² | conditioned | ISO 179/1eU | |
Zugfestigkeit | 50 MPa Show Supplier Material materials with Zugfestigkeit of 50 MPa | conditioned | ISO 527-1/-2 | |
95 MPa Show Supplier Material materials with Zugfestigkeit of 95 MPa | dry | ISO 527-1/-2 |
Thermisch
Property | Value | Condition | Thickness | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|---|
Entflammbarkeit | V-2 | dry | 1.5 mm | IEC 60695-11-10 | UL recognition :Yes | |
Glow Wire Flammability Index | 960 °C Show Supplier Material materials with Glow Wire Flammability Index of 960 °C | dry | 2 mm | IEC 60695-2-12 | ||
960 °C Show Supplier Material materials with Glow Wire Flammability Index of 960 °C | dry | 0.75 mm | IEC 60695-2-12 | |||
Glow Wire Ignition Temperature | 750 °C Show Supplier Material materials with Glow Wire Ignition Temperature of 750 °C | dry | 2 mm | IEC 60695-2-13 | ||
775 °C Show Supplier Material materials with Glow Wire Ignition Temperature of 775 °C | dry | 0.75 mm | IEC 60695-2-13 | |||
Relative temperature index, electrical | 130 °C Show Supplier Material materials with Relative temperature index, electrical of 130 °C | dry | 0.75 mm | UL746B | ||
Relative temperature index, mechanical strength | 130 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 130 °C | dry | 0.75 mm | UL746B | ||
Schmelzpunkt | 220 °C Show Supplier Material materials with Schmelzpunkt of 220 °C | dry | ISO 11357-1/-3 | 10°C/min | ||
Wärmeformbeständigkeitstemperatur | 180 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 180 °C | dry | ISO 75-1/-2 | 2 MPa |
Elektrisch
Property | Value | Condition | Testing Standard |
---|---|---|---|
Kriechstromfestigkeit | 525 V Show Supplier Material materials with Kriechstromfestigkeit of 525 V | dry | IEC 60112 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Application areas | Residual Current device, Contactors, Switch Base | |
Certifications | Yellow Card Available | |
Fillers | 30% Glass Fiber |