Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 1.13 g/cm³ Show Supplier Material materials with Dichte of 1.13 g/cm³ | dry | ISO 1183 |
Moisture absorption | 0.65 % Show Supplier Material materials with Moisture absorption of 0.65 % | dry | Sim. to ISO 62 |
Wasserabsorption | 0.2 % Show Supplier Material materials with Wasserabsorption of 0.2 % | dry | Sim. to ISO 62 |
Mechanisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Dehnung | 440 % Show Supplier Material materials with Dehnung of 440 % | dry | ISO 527-1/-2 | |
Elastizitätsmodul | 0.06 GPa Show Supplier Material materials with Elastizitätsmodul of 0.06 GPa | dry | ISO 527-1/-2 | |
Härte, Shore A | 88 [-] Show Supplier Material materials with Härte, Shore A of 88 [-] | dry | ISO 868 | 3s |
Zugfestigkeit | 10.6 MPa Show Supplier Material materials with Zugfestigkeit of 10.6 MPa | dry | ISO 527-1/-2 |
Thermisch
Elektrisch
Property | Value | Condition | Testing Standard |
---|---|---|---|
Durchschlagfestigkeit | 19.8 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 19.8 kV/mm | dry | IEC 60243-1 |
Volume resistivity | 8.3e+10 Ω·cm Show Supplier Material materials with Volume resistivity of 8.3e+10 Ω·cm | dry | IEC 62631-3-1 |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Schmelzvolumenflussrate | 230 °C | 4.3 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 4.3 cm³/10min | dry | ISO 1133 |
Technological properties
Property | ||
---|---|---|
Application areas | AC Cables, DC Cables | |
Certifications | Yellow Card Available |