Allgemein
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Dichte | 1.31 g/cm³ Show Supplier Material materials with Dichte of 1.31 g/cm³ | dry | ISO 1183 | |
Moisture absorption | 0.11 % Show Supplier Material materials with Moisture absorption of 0.11 % | dry | Sim. to ISO 62 | |
Wasserabsorption | 0.26 % Show Supplier Material materials with Wasserabsorption of 0.26 % | dry | ISO 62 | at 23°C after 24h |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Dehnung | 50 % Show Supplier Material materials with Dehnung of 50 % | dry | ISO 527-1/-2 | ||
Elastizitätsmodul | 0.2 GPa Show Supplier Material materials with Elastizitätsmodul of 0.2 GPa | dry | ISO 527-1/-2 | ||
Härte, Shore A | 97 [-] Show Supplier Material materials with Härte, Shore A of 97 [-] | dry | ISO 868 | 15s | |
98 [-] Show Supplier Material materials with Härte, Shore A of 98 [-] | dry | ISO 868 | 3s | ||
Härte, Shore D | 57.0 [-] Show Supplier Material materials with Härte, Shore D of 57.0 [-] | dry | ISO 868 | 3s | |
57.0 [-] Show Supplier Material materials with Härte, Shore D of 57.0 [-] | dry | ISO 868 | 15s | ||
Reißfestigkeit | 148 kN/m Show Supplier Material materials with Reißfestigkeit of 148 kN/m | dry | ISO 34-1; Method B | ||
Schlagfestigkeit, Charpy gekerbt | -30 °C | 4.8 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 4.8 kJ/m² | dry | ISO 179/1eA | |
Zugfestigkeit | 27 MPa Show Supplier Material materials with Zugfestigkeit of 27 MPa | dry | ISO 527-1/-2 |
Thermisch
Elektrisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Dielektrizitätskonstante | 3.5 [-] Show Supplier Material materials with Dielektrizitätskonstante of 3.5 [-] | dry | IEC 62631-2-1 | 1MHz |
4.2 [-] Show Supplier Material materials with Dielektrizitätskonstante of 4.2 [-] | dry | IEC 62631-2-1 | 100Hz | |
Verlustfaktor | 180 [-] Show Supplier Material materials with Verlustfaktor of 180 [-] | dry | IEC 62631-2-1 | 100Hz |
495 [-] Show Supplier Material materials with Verlustfaktor of 495 [-] | dry | IEC 62631-2-1 | 1MHz | |
Volume resistivity | 1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 62631-3-1 |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Schmelzvolumenflussrate | 230 °C | 17 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 17 cm³/10min | dry | ISO 1133 |
Technological properties
Property | ||
---|---|---|
Application areas | Wire and Cable Insulation |