Allgemein
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Dichte | 1.18 g/cm³ Show Supplier Material materials with Dichte of 1.18 g/cm³ | dry | ISO 1183 | |
Moisture absorption | 1.19 % Show Supplier Material materials with Moisture absorption of 1.19 % | dry | Sim. to ISO 62 | |
Wasserabsorption | 0.88 % Show Supplier Material materials with Wasserabsorption of 0.88 % | dry | ISO 62 | at 23°C after 24h |
Mechanisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Dehnung | 50 % Show Supplier Material materials with Dehnung of 50 % | dry | ISO 527-1/-2 | |
150 % Show Supplier Material materials with Dehnung of 150 % | dry | ISO 527-1/-2 | ||
Elastizitätsmodul | 0.14 GPa Show Supplier Material materials with Elastizitätsmodul of 0.14 GPa | dry | ISO 527-1/-2 | |
Härte, Shore A | 97 [-] Show Supplier Material materials with Härte, Shore A of 97 [-] | dry | ISO 868 | 3s |
97 [-] Show Supplier Material materials with Härte, Shore A of 97 [-] | dry | ISO 868 | 15s | |
Härte, Shore D | 51 [-] Show Supplier Material materials with Härte, Shore D of 51 [-] | dry | ISO 868 | 3s |
51 [-] Show Supplier Material materials with Härte, Shore D of 51 [-] | dry | ISO 868 | 15s | |
Reißfestigkeit | 123 kN/m Show Supplier Material materials with Reißfestigkeit of 123 kN/m | dry | ISO 34-1; Method B | |
Zugfestigkeit | 24 MPa Show Supplier Material materials with Zugfestigkeit of 24 MPa | dry | ISO 527-1/-2 |
Thermisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Glasübergangstemperatur | -78 °C Show Supplier Material materials with Glasübergangstemperatur of -78 °C | dry | ISO 11357-1/-2 | 10°C/min |
Koeffizient der thermischen Ausdehnung | 2.2e-06 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 2.2e-06 1/K | dry | ISO 11359-1/-2 | Parallel |
2.2e-06 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 2.2e-06 1/K | dry | ISO 11359-1/-2 | Normal | |
Schmelzpunkt | 204 °C Show Supplier Material materials with Schmelzpunkt of 204 °C | dry | ISO 11357-1/-3 | 10°C/min |
Vicat-Erweichungstemperatur | 54 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 54 °C | dry | ISO 306 | 50°C/h 50N |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Schmelzvolumenflussrate | 230 °C | 7 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 7 cm³/10min | dry | ISO 1133 |
Technological properties
Property |
---|