Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 1.13 g/cm³ Show Supplier Material materials with Dichte of 1.13 g/cm³ | dry | ISO 1183 |
Moisture absorption | 2.8 % Show Supplier Material materials with Moisture absorption of 2.8 % | dry | Sim. to ISO 62 |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Biegemodul | 2.6 GPa Show Supplier Material materials with Biegemodul of 2.6 GPa | dry | ISO 178 | |
Dehnung | 50 % Show Supplier Material materials with Dehnung of 50 % | dry | ISO 527-1/-2 | |
Elastizitätsmodul | 2.9 GPa Show Supplier Material materials with Elastizitätsmodul of 2.9 GPa | dry | ISO 527-1/-2 | |
Elongation at yield | 4.2 % Show Supplier Material materials with Elongation at yield of 4.2 % | dry | ISO 527-1/-2 | |
Flexural yield strength | 108 MPa Show Supplier Material materials with Flexural yield strength of 108 MPa | dry | ISO 178 | |
Schlagfestigkeit, Charpy gekerbt | 23 °C | 2.7 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 2.7 kJ/m² | dry | ISO 179/1eA |
Thermisch
Property | Value | Condition | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|
Schmelzpunkt | 220 °C Show Supplier Material materials with Schmelzpunkt of 220 °C | dry | ISO 11357-1/-3 | 10°C/min | |
Wärmeformbeständigkeitstemperatur | 60 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 60 °C | dry | ISO 75-1/-2 | 2 MPa | |
154 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 154 °C | dry | ISO 75-1/-2 | 0.45 MPa |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Schmelzvolumenflussrate | 230 °C | 8 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 8 cm³/10min | dry | ISO 1133 |
Technological properties
Property |
---|