Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 1.15 g/cm³ Show Supplier Material materials with Dichte of 1.15 g/cm³ | dry | ISO 1183 |
Moisture absorption | 2.2 % Show Supplier Material materials with Moisture absorption of 2.2 % | dry | Sim. to ISO 62 |
Wasserabsorption | 7.6 % Show Supplier Material materials with Wasserabsorption of 7.6 % | dry | Sim. to ISO 62 |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Dehnung | 5.5 % Show Supplier Material materials with Dehnung of 5.5 % | dry | ISO 527-1/-2 | |
15 % Show Supplier Material materials with Dehnung of 15 % | conditioned | ISO 527-1/-2 | ||
Elastizitätsmodul | 1.9 GPa Show Supplier Material materials with Elastizitätsmodul of 1.9 GPa | conditioned | ISO 527-1/-2 | |
3.7 GPa Show Supplier Material materials with Elastizitätsmodul of 3.7 GPa | dry | ISO 527-1/-2 | ||
Schlagfestigkeit, Charpy gekerbt | -30 °C | 4 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 4 kJ/m² | dry, conditioned | ISO 179/1eA |
23 °C | 15 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 15 kJ/m² | dry | ISO 179/1eA | |
23 °C | 22 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 22 kJ/m² | conditioned | ISO 179/1eA | |
Schlagzähigkeit, Charpy ungekerbt | -30 °C | 45 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 45 kJ/m² | dry, conditioned | ISO 179/1eU |
23 °C | 65 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 65 kJ/m² | dry | ISO 179/1eU | |
23 °C | 80 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 80 kJ/m² | conditioned | ISO 179/1eU | |
Zugfestigkeit | 50 MPa Show Supplier Material materials with Zugfestigkeit of 50 MPa | conditioned | ISO 527-1/-2 | |
85 MPa Show Supplier Material materials with Zugfestigkeit of 85 MPa | dry | ISO 527-1/-2 |
Thermisch
Property | Value | Condition | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|
Koeffizient der thermischen Ausdehnung | 3e-07 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 3e-07 1/K | dry | ISO 11359-1/-2 | Parallel | |
8e-07 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 8e-07 1/K | dry | ISO 11359-1/-2 | Normal | ||
Wärmeformbeständigkeitstemperatur | 125 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 125 °C | dry | ISO 75-1/-2 | 2 MPa | |
200 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 200 °C | dry | ISO 75-1/-2 | 0.45 MPa |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Schmelzvolumenflussrate | 275 °C | 23 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 23 cm³/10min | dry | ISO 1133 |
Technological properties
Property | ||
---|---|---|
Fillers | 8% Glass Fiber |