Allgemein
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Dichte | 1.41 g/cm³ Show Supplier Material materials with Dichte of 1.41 g/cm³ | dry | ISO 1183 | |
Moisture absorption | 2.6 % Show Supplier Material materials with Moisture absorption of 2.6 % | dry | Sim. to ISO 62 | |
Sauerstoffindex | 22 % Show Supplier Material materials with Sauerstoffindex of 22 % | dry | ISO 4589-1/-2 | |
Wasserabsorption | 2.65 % Show Supplier Material materials with Wasserabsorption of 2.65 % | dry | ISO 62 | at 23°C after 24h |
9.5 % Show Supplier Material materials with Wasserabsorption of 9.5 % | dry | Sim. to ISO 62 |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard | Thickness | Comment |
---|---|---|---|---|---|---|
Biegemodul | 5.5 GPa Show Supplier Material materials with Biegemodul of 5.5 GPa | conditioned | ISO 178 | |||
9.5 GPa Show Supplier Material materials with Biegemodul of 9.5 GPa | dry | ISO 178 | ||||
120 °C | 5.1 GPa Show Supplier Material materials with Biegemodul of 5.1 GPa | dry | ISO 178 | |||
160 °C | 4.9 GPa Show Supplier Material materials with Biegemodul of 4.9 GPa | dry | ISO 178 | |||
Dehnung | 2.5 % Show Supplier Material materials with Dehnung of 2.5 % | dry | ISO 527-1/-2 | |||
2.6 % Show Supplier Material materials with Dehnung of 2.6 % | dry | ISO 527-1/-2 | 1 mm | |||
5 % Show Supplier Material materials with Dehnung of 5 % | conditioned | ISO 527-1/-2 | ||||
5 % Show Supplier Material materials with Dehnung of 5 % | conditioned | ISO 527-1/-2 | ||||
120 °C | 5.5 % Show Supplier Material materials with Dehnung of 5.5 % | dry | ISO 527-1/-2 | |||
160 °C | 5.5 % Show Supplier Material materials with Dehnung of 5.5 % | dry | ISO 527-1/-2 | |||
180 °C | 5.5 % Show Supplier Material materials with Dehnung of 5.5 % | dry | ISO 527-1/-2 | |||
200 °C | 5.5 % Show Supplier Material materials with Dehnung of 5.5 % | dry | ISO 527-1/-2 | |||
Elastizitätsmodul | 6 GPa Show Supplier Material materials with Elastizitätsmodul of 6 GPa | conditioned | ISO 527-1/-2 | |||
6 GPa Show Supplier Material materials with Elastizitätsmodul of 6 GPa | conditioned | ISO 527-1/-2 | ||||
10 GPa Show Supplier Material materials with Elastizitätsmodul of 10 GPa | dry | ISO 527-1/-2 | ||||
10 GPa Show Supplier Material materials with Elastizitätsmodul of 10 GPa | dry | ISO 527-1/-2 | 1 mm | |||
120 °C | 5.3 GPa Show Supplier Material materials with Elastizitätsmodul of 5.3 GPa | dry | ISO 527-1/-2 | |||
160 °C | 4.8 GPa Show Supplier Material materials with Elastizitätsmodul of 4.8 GPa | dry | ISO 527-1/-2 | |||
180 °C | 4.5 GPa Show Supplier Material materials with Elastizitätsmodul of 4.5 GPa | dry | ISO 527-1/-2 | |||
200 °C | 4.3 GPa Show Supplier Material materials with Elastizitätsmodul of 4.3 GPa | dry | ISO 527-1/-2 | |||
Flexural yield strength | 160 MPa Show Supplier Material materials with Flexural yield strength of 160 MPa | conditioned | ISO 178 | |||
270 MPa Show Supplier Material materials with Flexural yield strength of 270 MPa | dry | ISO 178 | ||||
120 °C | 140 MPa Show Supplier Material materials with Flexural yield strength of 140 MPa | dry | ISO 178 | |||
160 °C | 125 MPa Show Supplier Material materials with Flexural yield strength of 125 MPa | dry | ISO 178 | |||
Schlagfestigkeit, Charpy gekerbt | -30 °C | 10 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 10 kJ/m² | dry, conditioned | ISO 179/1eA | ||
23 °C | 10 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 10 kJ/m² | dry | ISO 179/1eA | |||
23 °C | 15 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 15 kJ/m² | conditioned | ISO 179/1eA | |||
Schlagzähigkeit, Charpy ungekerbt | -30 °C | 60 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 60 kJ/m² | dry, conditioned | ISO 179/1eU | ||
23 °C | 60 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 60 kJ/m² | dry | ISO 179/1eU | |||
23 °C | 90 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 90 kJ/m² | conditioned | ISO 179/1eU | |||
Zugfestigkeit | 110 MPa Show Supplier Material materials with Zugfestigkeit of 110 MPa | conditioned | ISO 527-1/-2 | |||
115 MPa Show Supplier Material materials with Zugfestigkeit of 115 MPa | conditioned | ISO 527-1/-2 | at low thickness | |||
180 MPa Show Supplier Material materials with Zugfestigkeit of 180 MPa | dry | ISO 527-1/-2 | ||||
180 MPa Show Supplier Material materials with Zugfestigkeit of 180 MPa | dry | ISO 527-1/-2 | 1 mm | at low thickness | ||
120 °C | 105 MPa Show Supplier Material materials with Zugfestigkeit of 105 MPa | dry | ISO 527-1/-2 | |||
160 °C | 90 MPa Show Supplier Material materials with Zugfestigkeit of 90 MPa | dry | ISO 527-1/-2 | |||
180 °C | 85 MPa Show Supplier Material materials with Zugfestigkeit of 85 MPa | dry | ISO 527-1/-2 | |||
200 °C | 80 MPa Show Supplier Material materials with Zugfestigkeit of 80 MPa | dry | ISO 527-1/-2 |
Thermisch
Property | Value | Condition | Thickness | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|---|
Entflammbarkeit | HB | dry | 1.5 mm | IEC 60695-11-10 | UL recognition :Yes | |
Glasübergangstemperatur | 75 °C Show Supplier Material materials with Glasübergangstemperatur of 75 °C | dry | ISO 11357-1/-2 | 10°C/min | ||
Koeffizient der thermischen Ausdehnung | 2.5e-07 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 2.5e-07 1/K | dry | ISO 11359-1/-2 | Parallel | ||
6e-07 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 6e-07 1/K | dry | ISO 11359-1/-2 | Normal | |||
Relative temperature index, electrical | 65 °C Show Supplier Material materials with Relative temperature index, electrical of 65 °C | dry | 0.75 mm | UL746B | ||
Relative temperature index, mechanical impact | 65 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 65 °C | dry | 0.75 mm | UL746B | ||
Relative temperature index, mechanical strength | 65 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 65 °C | dry | 0.75 mm | UL746B | ||
Schmelzpunkt | 295 °C Show Supplier Material materials with Schmelzpunkt of 295 °C | dry | ISO 11357-1/-3 | 10°C/min | ||
Vicat-Erweichungstemperatur | 290 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 290 °C | dry | ISO 306 | 50°C/h 50N | ||
Wärmeformbeständigkeitstemperatur | 290 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 290 °C | dry | ISO 75-1/-2 | 2 MPa | ||
290 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 290 °C | dry | ISO 75-1/-2 | 0.45 MPa |
Elektrisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Dielektrizitätskonstante | 3.6 [-] Show Supplier Material materials with Dielektrizitätskonstante of 3.6 [-] | dry | IEC 60250 | 1GHz |
4 [-] Show Supplier Material materials with Dielektrizitätskonstante of 4 [-] | dry | IEC 62631-2-1 | 1MHz | |
4.4 [-] Show Supplier Material materials with Dielektrizitätskonstante of 4.4 [-] | dry | IEC 62631-2-1 | 100Hz | |
4.6 [-] Show Supplier Material materials with Dielektrizitätskonstante of 4.6 [-] | conditioned | IEC 62631-2-1 | 1MHz | |
12 [-] Show Supplier Material materials with Dielektrizitätskonstante of 12 [-] | conditioned | IEC 62631-2-1 | 100Hz | |
Durchschlagfestigkeit | 25 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 25 kV/mm | conditioned | IEC 60243-1 | |
30 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 30 kV/mm | dry | IEC 60243-1 | ||
Kriechstromfestigkeit | 550 V Show Supplier Material materials with Kriechstromfestigkeit of 550 V | dry | IEC 60112 | |
Surface resistivity | 1e+14 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+14 Ω/sq | conditioned | IEC 62631-3-2 | |
Verlustfaktor | 80 [-] Show Supplier Material materials with Verlustfaktor of 80 [-] | dry | IEC 62631-2-1 | 100Hz |
230 [-] Show Supplier Material materials with Verlustfaktor of 230 [-] | dry | IEC 62631-2-1 | 1MHz | |
300 [-] Show Supplier Material materials with Verlustfaktor of 300 [-] | dry | IEC 60250 | 1GHz | |
900 [-] Show Supplier Material materials with Verlustfaktor of 900 [-] | conditioned | IEC 62631-2-1 | 1MHz | |
1500 [-] Show Supplier Material materials with Verlustfaktor of 1500 [-] | conditioned | IEC 62631-2-1 | 100Hz | |
Volume resistivity | 1e+09 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+09 Ω·cm | conditioned | IEC 62631-3-1 | |
1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 62631-3-1 |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Schrumpfung | 0.5 % Show Supplier Material materials with Schrumpfung of 0.5 % | dry | Sim. to ISO 294-4 | Parallel |
1.3 % Show Supplier Material materials with Schrumpfung of 1.3 % | dry | Sim. to ISO 294-4 | Normal | |
Spiral flow length | 145 | dry | - | 1.0 mm 800 bar |
170 | dry | - | 1.0 mm 900 bar | |
195 | dry | - | 1.0 mm 1000 bar | |
86 | dry | - | 0.5mm 1200 bar | |
110 | dry | - | 0.5mm 1600 bar | |
132 | dry | - | 0.5mm 2000 bar | |
Viscosity number | 95 cm³/gr Show Supplier Material materials with Viscosity number of 95 cm³/gr | dry | ISO 307, 1157, 1628 |
Technological properties
Property | ||
---|---|---|
Certifications | Yellow Card Available | |
Fillers | 30% Glass Fiber |