Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 1.21 g/cm³ Show Supplier Material materials with Dichte of 1.21 g/cm³ | dry | ISO 1183 |
Mechanisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Dehnung | 215 % Show Supplier Material materials with Dehnung of 215 % | dry | ISO 527-1/-2 | |
Elastizitätsmodul | 0.2 GPa Show Supplier Material materials with Elastizitätsmodul of 0.2 GPa | dry | ISO 527-1/-2 | |
Härte, Shore D | 46 [-] Show Supplier Material materials with Härte, Shore D of 46 [-] | dry | ISO 868 | 3s |
Zugfestigkeit | 21.1 MPa Show Supplier Material materials with Zugfestigkeit of 21.1 MPa | dry | ISO 527-1/-2 |
Thermisch
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Schmelzvolumenflussrate | 230 °C | 10 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 10 cm³/10min | dry | ISO 1133 | |
Schrumpfung | 1.5 % Show Supplier Material materials with Schrumpfung of 1.5 % | dry | Sim. to ISO 294-4 | Parallel | |
1.6 % Show Supplier Material materials with Schrumpfung of 1.6 % | dry | Sim. to ISO 294-4 | Normal |
Technological properties
Property | ||
---|---|---|
Application areas | Spider Couplings |