Allgemein
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Bio-based content | 52 % Show Supplier Material materials with Bio-based content of 52 % | dry | ASTM D6866-12 Method B | |
Dichte | 1.1 g/cm³ Show Supplier Material materials with Dichte of 1.1 g/cm³ | dry | ISO 1183 | |
Moisture absorption | 0.04 % Show Supplier Material materials with Moisture absorption of 0.04 % | dry | Sim. to ISO 62 | |
Wasserabsorption | 0.14 % Show Supplier Material materials with Wasserabsorption of 0.14 % | dry | ISO 62 | at 23°C after 24h |
Mechanisch
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dehnung | 50 % Show Supplier Material materials with Dehnung of 50 % | dry | ISO 527-1/-2 |
Elastizitätsmodul | 0.04 GPa Show Supplier Material materials with Elastizitätsmodul of 0.04 GPa | dry | ISO 527-1/-2 |
Reißfestigkeit | 75 kN/m Show Supplier Material materials with Reißfestigkeit of 75 kN/m | dry | ISO 34-1; Method B |
Zugfestigkeit | 9 MPa Show Supplier Material materials with Zugfestigkeit of 9 MPa | dry | ISO 527-1/-2 |
Thermisch
Elektrisch
Property | Value | Condition | Testing Standard |
---|---|---|---|
Durchschlagfestigkeit | 20 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 20 kV/mm | dry | IEC 60243-1 |
Surface resistivity | 1e+15 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+15 Ω/sq | dry | IEC 62631-3-2 |
Volume resistivity | 1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 62631-3-1 |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Schmelzvolumenflussrate | 230 °C | 45 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 45 cm³/10min | dry | ISO 1133 |
Technological properties
Property |
---|