Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 1.44 g/cm³ Show Supplier Material materials with Dichte of 1.44 g/cm³ | dry | ISO 1183 |
Moisture absorption | 1.6 % Show Supplier Material materials with Moisture absorption of 1.6 % | dry | Sim. to ISO 62 |
Wasserabsorption | 4.3 % Show Supplier Material materials with Wasserabsorption of 4.3 % | dry | Sim. to ISO 62 |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Dehnung | 2.8 % Show Supplier Material materials with Dehnung of 2.8 % | dry | ISO 527-1/-2 | |
Elastizitätsmodul | 11 GPa Show Supplier Material materials with Elastizitätsmodul of 11 GPa | dry | ISO 527-1/-2 | |
Schlagfestigkeit, Charpy gekerbt | 23 °C | 9 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 9 kJ/m² | dry | ISO 179/1eA |
Schlagzähigkeit, Charpy ungekerbt | 23 °C | 63 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 63 kJ/m² | dry | ISO 179/1eU |
Zugfestigkeit | 150 MPa Show Supplier Material materials with Zugfestigkeit of 150 MPa | dry | ISO 527-1/-2 |
Thermisch
Property | Value | Condition | Thickness | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|---|
Entflammbarkeit | V-0 | dry | 1.5 mm | IEC 60695-11-10 | UL recognition :Yes | |
Relative temperature index, electrical | 130 °C Show Supplier Material materials with Relative temperature index, electrical of 130 °C | dry | 0.4 mm | UL746B | ||
Relative temperature index, mechanical impact | 110 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 110 °C | dry | 0.4 mm | UL746B | ||
Relative temperature index, mechanical strength | 115 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 115 °C | dry | 0.4 mm | UL746B | ||
Schmelzpunkt | 260 °C Show Supplier Material materials with Schmelzpunkt of 260 °C | dry | ISO 11357-1/-3 | 10°C/min | ||
Wärmeformbeständigkeitstemperatur | 245 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 245 °C | dry | ISO 75-1/-2 | 2 MPa |
Elektrisch
Property | Value | Condition | Testing Standard |
---|---|---|---|
Durchschlagfestigkeit | 32 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 32 kV/mm | conditioned | IEC 60243-1 |
36 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 36 kV/mm | dry | IEC 60243-1 | |
Kriechstromfestigkeit | 600 V Show Supplier Material materials with Kriechstromfestigkeit of 600 V | dry | IEC 60112 |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Schrumpfung | 0.2 % Show Supplier Material materials with Schrumpfung of 0.2 % | dry | Sim. to ISO 294-4 | Parallel |
0.8 % Show Supplier Material materials with Schrumpfung of 0.8 % | dry | Sim. to ISO 294-4 | Normal | |
Spiral flow length | 73 | dry | - | 1.0 mm 800 bar |
81 | dry | - | 1.0 mm 900 bar | |
89 | dry | - | 1.0 mm 1000 bar |
Technological properties
Property | ||
---|---|---|
Application areas | MCCB Housings, Industrial Control Gear | |
Certifications | Yellow Card Available | |
Fillers | 30% Glass Fiber |