Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 1.1 g/cm³ Show Supplier Material materials with Dichte of 1.1 g/cm³ | dry | ISO 1183 |
Moisture absorption | 0.45 % Show Supplier Material materials with Moisture absorption of 0.45 % | dry | Sim. to ISO 62 |
Wasserabsorption | 0.16 % Show Supplier Material materials with Wasserabsorption of 0.16 % | dry | Sim. to ISO 62 |
Mechanisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Dehnung | 550 % Show Supplier Material materials with Dehnung of 550 % | dry | ISO 527-1/-2 | |
Elastizitätsmodul | 0.04 GPa Show Supplier Material materials with Elastizitätsmodul of 0.04 GPa | dry | ISO 527-1/-2 | |
Härte, Shore A | 82 [-] Show Supplier Material materials with Härte, Shore A of 82 [-] | dry | ISO 868 | 3s |
Zugfestigkeit | 8.8 MPa Show Supplier Material materials with Zugfestigkeit of 8.8 MPa | dry | ISO 527-1/-2 |
Thermisch
Elektrisch
Property | Value | Condition | Testing Standard |
---|---|---|---|
Durchschlagfestigkeit | 21.5 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 21.5 kV/mm | dry | IEC 60243-1 |
Volume resistivity | 8.4e+11 Ω·cm Show Supplier Material materials with Volume resistivity of 8.4e+11 Ω·cm | dry | IEC 62631-3-1 |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Schmelzvolumenflussrate | 230 °C | 13.8 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 13.8 cm³/10min | dry | ISO 1133 |
Technological properties
Property | ||
---|---|---|
Certifications | Yellow Card Available |