Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 1.48 g/cm³ Show Supplier Material materials with Dichte of 1.48 g/cm³ | dry | ISO 1183 |
Moisture absorption | 0.15 % Show Supplier Material materials with Moisture absorption of 0.15 % | dry | Sim. to ISO 62 |
Wasserabsorption | 0.35 % Show Supplier Material materials with Wasserabsorption of 0.35 % | dry | Sim. to ISO 62 |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Dehnung | 2.2 % Show Supplier Material materials with Dehnung of 2.2 % | dry | ISO 527-1/-2 | |
Elastizitätsmodul | 4.5 GPa Show Supplier Material materials with Elastizitätsmodul of 4.5 GPa | dry | ISO 527-1/-2 | |
Schlagfestigkeit, Charpy gekerbt | 23 °C | 2 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 2 kJ/m² | dry | ISO 179/1eA |
Schlagzähigkeit, Charpy ungekerbt | 23 °C | 30 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 30 kJ/m² | dry | ISO 179/1eU |
Zugfestigkeit | 55.0 MPa Show Supplier Material materials with Zugfestigkeit of 55.0 MPa | dry | ISO 527-1/-2 |
Thermisch
Property | Value | Condition | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|
Schmelzpunkt | 225 °C Show Supplier Material materials with Schmelzpunkt of 225 °C | dry | ISO 11357-1/-3 | 10°C/min | |
Wärmeformbeständigkeitstemperatur | 100 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 100 °C | dry | ISO 75-1/-2 | 2 MPa | |
195 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 195 °C | dry | ISO 75-1/-2 | 0.45 MPa |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Schmelzvolumenflussrate | 270 °C | 34 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 34 cm³/10min | dry | ISO 1133 | |
Schrumpfung | 1.4 % Show Supplier Material materials with Schrumpfung of 1.4 % | dry | Sim. to ISO 294-4 | Parallel | |
1.7 % Show Supplier Material materials with Schrumpfung of 1.7 % | dry | Sim. to ISO 294-4 | Normal |
Technological properties
Property | ||
---|---|---|
Fillers | 20% Mineral Powder |