Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 1.53 g/cm³ Show Supplier Material materials with Dichte of 1.53 g/cm³ | dry | ISO 1183 |
Moisture absorption | 1.7 % Show Supplier Material materials with Moisture absorption of 1.7 % | dry | Sim. to ISO 62 |
Wasserabsorption | 6.2 % Show Supplier Material materials with Wasserabsorption of 6.2 % | dry | Sim. to ISO 62 |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Dehnung | 2.5 % Show Supplier Material materials with Dehnung of 2.5 % | dry | ISO 527-1/-2 | |
4 % Show Supplier Material materials with Dehnung of 4 % | conditioned | ISO 527-1/-2 | ||
Elastizitätsmodul | 3.5 GPa Show Supplier Material materials with Elastizitätsmodul of 3.5 GPa | conditioned | ISO 527-1/-2 | |
6.6 GPa Show Supplier Material materials with Elastizitätsmodul of 6.6 GPa | dry | ISO 527-1/-2 | ||
Schlagfestigkeit, Charpy gekerbt | -30 °C | 2 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 2 kJ/m² | dry, conditioned | ISO 179/1eA |
23 °C | 2 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 2 kJ/m² | dry, conditioned | ISO 179/1eA | |
Schlagzähigkeit, Charpy ungekerbt | -30 °C | 35 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 35 kJ/m² | dry, conditioned | ISO 179/1eU |
23 °C | 35 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 35 kJ/m² | dry | ISO 179/1eU | |
23 °C | 60 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 60 kJ/m² | conditioned | ISO 179/1eU | |
Zugfestigkeit | 40 MPa Show Supplier Material materials with Zugfestigkeit of 40 MPa | conditioned | ISO 527-1/-2 | |
70 MPa Show Supplier Material materials with Zugfestigkeit of 70 MPa | dry | ISO 527-1/-2 |
Thermisch
Property | Value | Condition | Thickness | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|---|
Entflammbarkeit | V-2 | dry | 1.5 mm | IEC 60695-11-10 | UL recognition :Yes | |
Glow Wire Flammability Index | 960 °C Show Supplier Material materials with Glow Wire Flammability Index of 960 °C | dry | 1 mm | IEC 60695-2-12 | ||
960 °C Show Supplier Material materials with Glow Wire Flammability Index of 960 °C | dry | 3 mm | IEC 60695-2-12 | |||
Glow Wire Ignition Temperature | 725 °C Show Supplier Material materials with Glow Wire Ignition Temperature of 725 °C | dry | 0.75 mm | IEC 60695-2-13 | ||
775 °C Show Supplier Material materials with Glow Wire Ignition Temperature of 775 °C | dry | 3 mm | IEC 60695-2-13 | |||
Koeffizient der thermischen Ausdehnung | 5e-07 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 5e-07 1/K | dry | ISO 11359-1/-2 | Parallel | ||
5e-07 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 5e-07 1/K | dry | ISO 11359-1/-2 | Normal | |||
Relative temperature index, electrical | 140 °C Show Supplier Material materials with Relative temperature index, electrical of 140 °C | dry | 0.75 mm | UL746B | ||
Relative temperature index, mechanical impact | 110 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 110 °C | dry | 0.75 mm | UL746B | ||
Relative temperature index, mechanical strength | 140 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 140 °C | dry | 0.75 mm | UL746B | ||
Schmelzpunkt | 220 °C Show Supplier Material materials with Schmelzpunkt of 220 °C | dry | ISO 11357-1/-3 | 10°C/min | ||
Wärmeformbeständigkeitstemperatur | 120 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 120 °C | dry | ISO 75-1/-2 | 2 MPa | ||
205 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 205 °C | dry | ISO 75-1/-2 | 0.45 MPa |
Elektrisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Dielektrizitätskonstante | 3.2 [-] Show Supplier Material materials with Dielektrizitätskonstante of 3.2 [-] | dry | IEC 62631-2-1 | 1MHz |
3.6 [-] Show Supplier Material materials with Dielektrizitätskonstante of 3.6 [-] | dry | IEC 62631-2-1 | 100Hz | |
3.7 [-] Show Supplier Material materials with Dielektrizitätskonstante of 3.7 [-] | conditioned | IEC 62631-2-1 | 1MHz | |
10 [-] Show Supplier Material materials with Dielektrizitätskonstante of 10 [-] | conditioned | IEC 62631-2-1 | 100Hz | |
Durchschlagfestigkeit | 25 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 25 kV/mm | conditioned | IEC 60243-1 | |
30 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 30 kV/mm | dry | IEC 60243-1 | ||
Kriechstromfestigkeit | 375 V Show Supplier Material materials with Kriechstromfestigkeit of 375 V | dry, conditioned | IEC 60112 | |
Surface resistivity | 1e+14 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+14 Ω/sq | conditioned | IEC 62631-3-2 | |
Verlustfaktor | 85 [-] Show Supplier Material materials with Verlustfaktor of 85 [-] | dry | IEC 62631-2-1 | 100Hz |
140 [-] Show Supplier Material materials with Verlustfaktor of 140 [-] | dry | IEC 62631-2-1 | 1MHz | |
900 [-] Show Supplier Material materials with Verlustfaktor of 900 [-] | conditioned | IEC 62631-2-1 | 1MHz | |
3000 [-] Show Supplier Material materials with Verlustfaktor of 3000 [-] | conditioned | IEC 62631-2-1 | 100Hz | |
Volume resistivity | 1e+11 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+11 Ω·cm | conditioned | IEC 62631-3-1 | |
1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 62631-3-1 |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Schmelzvolumenflussrate | 250 °C | 22 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 22 cm³/10min | dry | ISO 1133 | |
Schrumpfung | 0.63 % Show Supplier Material materials with Schrumpfung of 0.63 % | dry | ISO 294-4 | Parallel | |
0.63 % Show Supplier Material materials with Schrumpfung of 0.63 % | dry | ISO 294-4 | Normal |
Technological properties
Property | ||
---|---|---|
Application areas | Miniature Circuit Breakers | |
Certifications | Yellow Card Available | |
Fillers | 30% Mineral Powder |