Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 1.39 g/cm³ Show Supplier Material materials with Dichte of 1.39 g/cm³ | dry | ISO 1183 |
Moisture absorption | 0.3 % Show Supplier Material materials with Moisture absorption of 0.3 % | dry | Sim. to ISO 62 |
Mechanisch
Thermisch
Elektrisch
Property | Value | Condition | Testing Standard |
---|---|---|---|
Volume resistivity | 1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 62631-3-1 |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Schrumpfung | 1.6 % Show Supplier Material materials with Schrumpfung of 1.6 % | dry | ISO 294-4 | Parallel |
1.6 % Show Supplier Material materials with Schrumpfung of 1.6 % | dry | ISO 294-4 | Normal | |
Viscosity number | 85 cm³/gr Show Supplier Material materials with Viscosity number of 85 cm³/gr | dry | ISO 307, 1157, 1628 |
Technological properties
Property | ||
---|---|---|
Certifications | Food Contact |