Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 1.39 g/cm³ Show Supplier Material materials with Dichte of 1.39 g/cm³ | dry | ISO 1183 |
Moisture absorption | 1.65 % Show Supplier Material materials with Moisture absorption of 1.65 % | dry | Sim. to ISO 62 |
Wasserabsorption | 5.8 % Show Supplier Material materials with Wasserabsorption of 5.8 % | dry | Sim. to ISO 62 |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Biegemodul | 9.1 GPa Show Supplier Material materials with Biegemodul of 9.1 GPa | dry | ISO 178 | |
Dehnung | 3 % Show Supplier Material materials with Dehnung of 3 % | dry | ISO 527-1/-2 | |
5 % Show Supplier Material materials with Dehnung of 5 % | conditioned | ISO 527-1/-2 | ||
Elastizitätsmodul | 6.5 GPa Show Supplier Material materials with Elastizitätsmodul of 6.5 GPa | conditioned | ISO 527-1/-2 | |
10.5 GPa Show Supplier Material materials with Elastizitätsmodul of 10.5 GPa | dry | ISO 527-1/-2 | ||
Schlagfestigkeit, Charpy gekerbt | 23 °C | 9.5 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 9.5 kJ/m² | dry | ISO 179/1eA |
Zugfestigkeit | 120 MPa Show Supplier Material materials with Zugfestigkeit of 120 MPa | conditioned | ISO 527-1/-2 | |
170 MPa Show Supplier Material materials with Zugfestigkeit of 170 MPa | dry | ISO 527-1/-2 |
Thermisch
Property | Value | Condition | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|
Schmelzpunkt | 220 °C Show Supplier Material materials with Schmelzpunkt of 220 °C | dry | ISO 11357-1/-3 | 10°C/min | |
Wärmeformbeständigkeitstemperatur | 210 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 210 °C | dry | ISO 75-1/-2 | 2 MPa | |
220 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 220 °C | dry | ISO 75-1/-2 | 0.45 MPa |
Technological properties
Property | ||
---|---|---|
Fillers | 33% Glass Fiber |