Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 1.63 g/cm³ Show Supplier Material materials with Dichte of 1.63 g/cm³ | dry | ISO 1183 |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Biegemodul | 11.5 GPa Show Supplier Material materials with Biegemodul of 11.5 GPa | dry | ISO 178 | |
Dehnung | 3 % Show Supplier Material materials with Dehnung of 3 % | dry | ISO 527-1/-2 | |
Elastizitätsmodul | 13 GPa Show Supplier Material materials with Elastizitätsmodul of 13 GPa | dry | ISO 527-1/-2 | |
Flexural yield strength | 300 MPa Show Supplier Material materials with Flexural yield strength of 300 MPa | dry | ISO 178 | |
Schlagfestigkeit, Charpy gekerbt | 23 °C | 14.0 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 14.0 kJ/m² | dry | ISO 179/1eA |
Zugfestigkeit | 210 MPa Show Supplier Material materials with Zugfestigkeit of 210 MPa | dry | ISO 527-1/-2 |
Thermisch
Property | Value | Condition | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|
Glasübergangstemperatur | 75 °C Show Supplier Material materials with Glasübergangstemperatur of 75 °C | dry | ISO 11357-1/-2 | 10°C/min | |
Schmelzpunkt | 290 °C Show Supplier Material materials with Schmelzpunkt of 290 °C | dry | ISO 11357-1/-3 | 10°C/min | |
Vicat-Erweichungstemperatur | 285 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 285 °C | dry | ISO 306 | 50°C/h 50N | |
Wärmeformbeständigkeitstemperatur | 285 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 285 °C | dry | ISO 75-1/-2 | 2 MPa | |
285 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 285 °C | dry | ISO 75-1/-2 | 0.45 MPa |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Schrumpfung | 0.6 % Show Supplier Material materials with Schrumpfung of 0.6 % | dry | Sim. to ISO 294-4 | Parallel |
1.1 % Show Supplier Material materials with Schrumpfung of 1.1 % | dry | Sim. to ISO 294-4 | Normal | |
Viscosity number | 145 cm³/gr Show Supplier Material materials with Viscosity number of 145 cm³/gr | dry | ISO 307, 1157, 1628 |
Technological properties
Property | ||
---|---|---|
Fillers | 40% Glass Fiber and PTFE |