Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 1.33 g/cm³ Show Supplier Material materials with Dichte of 1.33 g/cm³ | dry | ISO 1183 |
Moisture absorption | 1.8 % Show Supplier Material materials with Moisture absorption of 1.8 % | dry | Sim. to ISO 62 |
Mechanisch
Property | Value | Condition | Testing Standard |
---|---|---|---|
Biegemodul | 4.4 GPa Show Supplier Material materials with Biegemodul of 4.4 GPa | conditioned | ISO 178 |
7.1 GPa Show Supplier Material materials with Biegemodul of 7.1 GPa | dry | ISO 178 | |
Dehnung | 7 % Show Supplier Material materials with Dehnung of 7 % | dry | ISO 527-1/-2 |
9 % Show Supplier Material materials with Dehnung of 9 % | conditioned | ISO 527-1/-2 | |
Flexural yield strength | 125 MPa Show Supplier Material materials with Flexural yield strength of 125 MPa | conditioned | ISO 178 |
190 MPa Show Supplier Material materials with Flexural yield strength of 190 MPa | dry | ISO 178 | |
Zugfestigkeit | 88 MPa Show Supplier Material materials with Zugfestigkeit of 88 MPa | conditioned | ISO 527-1/-2 |
135 MPa Show Supplier Material materials with Zugfestigkeit of 135 MPa | dry | ISO 527-1/-2 |
Thermisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Schmelzpunkt | 220 °C Show Supplier Material materials with Schmelzpunkt of 220 °C | dry | ISO 11357-1/-3 | 10°C/min |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Schmelzvolumenflussrate | 250 °C | 14.0 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 14.0 cm³/10min | dry | ISO 1133 |
Technological properties
Property | ||
---|---|---|
Fillers | 30% Glass Fiber |