Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 1.73 g/cm³ Show Supplier Material materials with Dichte of 1.73 g/cm³ | dry | ISO 1183 |
Moisture absorption | 0.12 % Show Supplier Material materials with Moisture absorption of 0.12 % | dry | Sim. to ISO 62 |
Sauerstoffindex | 36 % Show Supplier Material materials with Sauerstoffindex of 36 % | dry | ISO 4589-1/-2 |
Wasserabsorption | 0.4 % Show Supplier Material materials with Wasserabsorption of 0.4 % | dry | Sim. to ISO 62 |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Dehnung | 2 % Show Supplier Material materials with Dehnung of 2 % | dry | ISO 527-1/-2 | |
Elastizitätsmodul | 13 GPa Show Supplier Material materials with Elastizitätsmodul of 13 GPa | dry | ISO 527-1/-2 | |
Schlagfestigkeit, Charpy gekerbt | -30 °C | 8 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 8 kJ/m² | dry | ISO 179/1eA |
23 °C | 8 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 8 kJ/m² | dry | ISO 179/1eA | |
Schlagzähigkeit, Charpy ungekerbt | -30 °C | 35 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 35 kJ/m² | dry | ISO 179/1eU |
23 °C | 35 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 35 kJ/m² | dry | ISO 179/1eU | |
Zugfestigkeit | 160 MPa Show Supplier Material materials with Zugfestigkeit of 160 MPa | dry | ISO 527-1/-2 |
Thermisch
Property | Value | Condition | Thickness | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|---|
Entflammbarkeit | V-0 | dry | 1.5 mm | IEC 60695-11-10 | UL recognition :Yes | |
Koeffizient der thermischen Ausdehnung | 2e-07 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 2e-07 1/K | dry | ISO 11359-1/-2 | Parallel | ||
6.5e-07 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 6.5e-07 1/K | dry | ISO 11359-1/-2 | Normal | |||
Relative temperature index, electrical | 150 °C Show Supplier Material materials with Relative temperature index, electrical of 150 °C | dry | 0.71 mm | UL746B | ||
Relative temperature index, mechanical impact | 125 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 125 °C | dry | 0.71 mm | UL746B | ||
Relative temperature index, mechanical strength | 140 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 140 °C | dry | 0.71 mm | UL746B | ||
Schmelzpunkt | 255 °C Show Supplier Material materials with Schmelzpunkt of 255 °C | dry | ISO 11357-1/-3 | 10°C/min | ||
Temperaturleitfähigkeit | 8.67e-08 mm²/s Show Supplier Material materials with Temperaturleitfähigkeit of 8.67e-08 mm²/s | dry | - | |||
Wärmeformbeständigkeitstemperatur | 220 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 220 °C | dry | ISO 75-1/-2 | 2 MPa | ||
240 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 240 °C | dry | ISO 75-1/-2 | 0.45 MPa |
Elektrisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Dielektrizitätskonstante | 3.4 [-] Show Supplier Material materials with Dielektrizitätskonstante of 3.4 [-] | dry | IEC 62631-2-1 | 1MHz |
3.7 [-] Show Supplier Material materials with Dielektrizitätskonstante of 3.7 [-] | dry | IEC 62631-2-1 | 100Hz | |
Durchschlagfestigkeit | 29.0 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 29.0 kV/mm | dry | IEC 60243-1 | |
Kriechstromfestigkeit | 225 V Show Supplier Material materials with Kriechstromfestigkeit of 225 V | dry | IEC 60112 | |
Verlustfaktor | 10 [-] Show Supplier Material materials with Verlustfaktor of 10 [-] | dry | IEC 62631-2-1 | 100Hz |
120 [-] Show Supplier Material materials with Verlustfaktor of 120 [-] | dry | IEC 62631-2-1 | 1MHz | |
Volume resistivity | 1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 62631-3-1 |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Density of melt | 1350 g/cm³ Show Supplier Material materials with Density of melt of 1350 g/cm³ | dry | - | |
Schrumpfung | 0.5 % Show Supplier Material materials with Schrumpfung of 0.5 % | dry | ISO 294-4 | Parallel |
1 % Show Supplier Material materials with Schrumpfung of 1 % | dry | ISO 294-4 | Normal | |
Specific heat capacity melt | 1670 J/(kg·K) Show Supplier Material materials with Specific heat capacity melt of 1670 J/(kg·K) | dry | - | |
Thermal conductivity of melt | 0.195 W/(m·K) Show Supplier Material materials with Thermal conductivity of melt of 0.195 W/(m·K) | dry | - |
Technological properties
Property | ||
---|---|---|
Certifications | Yellow Card Available | |
Fillers | 33% Glass Fiber |