Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 1.24 g/cm³ Show Supplier Material materials with Dichte of 1.24 g/cm³ | dry | ISO 1183 |
Mechanisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Dehnung | 50 % Show Supplier Material materials with Dehnung of 50 % | dry | ISO 527-1/-2 | |
592 % Show Supplier Material materials with Dehnung of 592 % | dry | ISO 527-1/-2 | ||
Elastizitätsmodul | 0.14 GPa Show Supplier Material materials with Elastizitätsmodul of 0.14 GPa | dry | ISO 527-1/-2 | |
Härte, Shore D | 52 [-] Show Supplier Material materials with Härte, Shore D of 52 [-] | dry | ISO 868 | 3s |
Zugfestigkeit | 32 MPa Show Supplier Material materials with Zugfestigkeit of 32 MPa | dry | ISO 527-1/-2 | |
67 MPa Show Supplier Material materials with Zugfestigkeit of 67 MPa | dry | ISO 527-1/-2 | Normal |
Thermisch
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Schmelzmassenflussrate | 230 °C | 15 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 15 g/10min | dry | ISO 1133 |
Technological properties
Property | ||
---|---|---|
Application areas | Clean Air Inlet Ducts, Hot Charged Air Ducts |