Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 1.18 g/cm³ Show Supplier Material materials with Dichte of 1.18 g/cm³ | dry | ISO 1183 |
Mechanisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Dehnung | 160 % Show Supplier Material materials with Dehnung of 160 % | dry | ISO 527-1/-2 | |
760 % Show Supplier Material materials with Dehnung of 760 % | dry | ISO 527-1/-2 | ||
Elastizitätsmodul | 0.07 GPa Show Supplier Material materials with Elastizitätsmodul of 0.07 GPa | dry | ISO 527-1/-2 | |
Härte, Shore D | 37 [-] Show Supplier Material materials with Härte, Shore D of 37 [-] | dry | ISO 868 | 3s |
Reißfestigkeit | 91 kN/m Show Supplier Material materials with Reißfestigkeit of 91 kN/m | dry | ISO 34-1; Method B | |
104 kN/m Show Supplier Material materials with Reißfestigkeit of 104 kN/m | dry | ISO 34-1; Method B | ||
Zugfestigkeit | 16 MPa Show Supplier Material materials with Zugfestigkeit of 16 MPa | dry | ISO 527-1/-2 | |
27 MPa Show Supplier Material materials with Zugfestigkeit of 27 MPa | dry | ISO 527-1/-2 | Normal |
Thermisch
Property | Value | Condition | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|
Glasübergangstemperatur | -60 °C Show Supplier Material materials with Glasübergangstemperatur of -60 °C | dry | ISO 11357-1/-2 | 10°C/min | |
Schmelzpunkt | 212 °C Show Supplier Material materials with Schmelzpunkt of 212 °C | dry | ISO 11357-1/-3 | 10°C/min | |
Wärmeformbeständigkeitstemperatur | 65 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 65 °C | dry | ISO 75-1/-2 | 0.45 MPa |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Schmelzvolumenflussrate | 230 °C | 11 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 11 cm³/10min | dry | ISO 1133 | |
Schrumpfung | 1.5 % Show Supplier Material materials with Schrumpfung of 1.5 % | dry | Sim. to ISO 294-4 | Parallel | |
2.3 % Show Supplier Material materials with Schrumpfung of 2.3 % | dry | Sim. to ISO 294-4 | Normal |
Technological properties
Property | ||
---|---|---|
Application areas | Boots and Bellows |