Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 1.13 g/cm³ Show Supplier Material materials with Dichte of 1.13 g/cm³ | dry | ISO 1183 |
Moisture absorption | 2.8 % Show Supplier Material materials with Moisture absorption of 2.8 % | dry | Sim. to ISO 62 |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Biegemodul | 2.6 GPa Show Supplier Material materials with Biegemodul of 2.6 GPa | dry | ISO 178 | |
Dehnung | 50 % Show Supplier Material materials with Dehnung of 50 % | dry | ISO 527-1/-2 | |
Elastizitätsmodul | 2.8 GPa Show Supplier Material materials with Elastizitätsmodul of 2.8 GPa | dry | ISO 527-1/-2 | |
Flexural yield strength | 106 MPa Show Supplier Material materials with Flexural yield strength of 106 MPa | dry | ISO 178 | |
Schlagfestigkeit, Charpy gekerbt | -30 °C | 2.4 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 2.4 kJ/m² | dry | ISO 179/1eA |
23 °C | 4.8 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 4.8 kJ/m² | dry | ISO 179/1eA |
Thermisch
Property | Value | Condition | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|
Schmelzpunkt | 220 °C Show Supplier Material materials with Schmelzpunkt of 220 °C | dry | ISO 11357-1/-3 | 10°C/min | |
Wärmeformbeständigkeitstemperatur | 56 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 56 °C | dry | ISO 75-1/-2 | 2 MPa | |
153 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 153 °C | dry | ISO 75-1/-2 | 0.45 MPa |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Schmelzmassenflussrate | 230 °C | 39 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 39 g/10min | dry | ISO 1133 | |
Schmelzvolumenflussrate | 230 °C | 38 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 38 cm³/10min | dry | ISO 1133 | |
Schrumpfung | 1.4 % Show Supplier Material materials with Schrumpfung of 1.4 % | dry | ISO 294-4 | Parallel | |
1.4 % Show Supplier Material materials with Schrumpfung of 1.4 % | dry | ISO 294-4 | Normal | ||
Viscosity number | 125 cm³/gr Show Supplier Material materials with Viscosity number of 125 cm³/gr | dry | ISO 307, 1157, 1628 |
Technological properties
Property |
---|