Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 1.36 g/cm³ Show Supplier Material materials with Dichte of 1.36 g/cm³ | dry | ISO 1183 |
Moisture absorption | 2 % Show Supplier Material materials with Moisture absorption of 2 % | dry | Sim. to ISO 62 |
Wasserabsorption | 6.8 % Show Supplier Material materials with Wasserabsorption of 6.8 % | dry | Sim. to ISO 62 |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Dehnung | 2.5 % Show Supplier Material materials with Dehnung of 2.5 % | dry | ISO 527-1/-2 | |
25 % Show Supplier Material materials with Dehnung of 25 % | conditioned | ISO 527-1/-2 | ||
Elastizitätsmodul | 3 GPa Show Supplier Material materials with Elastizitätsmodul of 3 GPa | conditioned | ISO 527-1/-2 | |
7 GPa Show Supplier Material materials with Elastizitätsmodul of 7 GPa | dry | ISO 527-1/-2 | ||
Schlagfestigkeit, Charpy gekerbt | -30 °C | 3 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 3 kJ/m² | dry, conditioned | ISO 179/1eA |
23 °C | 3 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 3 kJ/m² | dry | ISO 179/1eA | |
23 °C | 7 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 7 kJ/m² | conditioned | ISO 179/1eA | |
Schlagzähigkeit, Charpy ungekerbt | -30 °C | 35 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 35 kJ/m² | dry, conditioned | ISO 179/1eU |
23 °C | 40 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 40 kJ/m² | dry | ISO 179/1eU | |
23 °C | 50 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 50 kJ/m² | conditioned | ISO 179/1eU | |
Zugfestigkeit | 45 MPa Show Supplier Material materials with Zugfestigkeit of 45 MPa | conditioned | ISO 527-1/-2 | |
90 MPa Show Supplier Material materials with Zugfestigkeit of 90 MPa | dry | ISO 527-1/-2 |
Thermisch
Property | Value | Condition | Thickness | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|---|
Entflammbarkeit | V-2 | dry | 1.5 mm | IEC 60695-11-10 | UL recognition :Yes | |
Relative temperature index, electrical | 65 °C Show Supplier Material materials with Relative temperature index, electrical of 65 °C | dry | 0.75 mm | UL746B | ||
Relative temperature index, mechanical impact | 65 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 65 °C | dry | 0.75 mm | UL746B | ||
Relative temperature index, mechanical strength | 65 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 65 °C | dry | 0.75 mm | UL746B | ||
Schmelzpunkt | 220 °C Show Supplier Material materials with Schmelzpunkt of 220 °C | dry | ISO 11357-1/-3 | 10°C/min | ||
Temperaturleitfähigkeit | 1.28e-07 mm²/s Show Supplier Material materials with Temperaturleitfähigkeit of 1.28e-07 mm²/s | dry | - | |||
Wärmeformbeständigkeitstemperatur | 190 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 190 °C | dry | ISO 75-1/-2 | 2 MPa | ||
210 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 210 °C | dry | ISO 75-1/-2 | 0.45 MPa |
Elektrisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Dielektrizitätskonstante | 3.8 [-] Show Supplier Material materials with Dielektrizitätskonstante of 3.8 [-] | dry | IEC 62631-2-1 | 1MHz |
3.9 [-] Show Supplier Material materials with Dielektrizitätskonstante of 3.9 [-] | conditioned | IEC 62631-2-1 | 1MHz | |
4.2 [-] Show Supplier Material materials with Dielektrizitätskonstante of 4.2 [-] | dry | IEC 62631-2-1 | 100Hz | |
10 [-] Show Supplier Material materials with Dielektrizitätskonstante of 10 [-] | conditioned | IEC 62631-2-1 | 100Hz | |
Durchschlagfestigkeit | 25 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 25 kV/mm | conditioned | IEC 60243-1 | |
30 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 30 kV/mm | dry | IEC 60243-1 | ||
Kriechstromfestigkeit | 475 V Show Supplier Material materials with Kriechstromfestigkeit of 475 V | dry, conditioned | IEC 60112 | |
Surface resistivity | 1e+14 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+14 Ω/sq | conditioned | IEC 62631-3-2 | |
Verlustfaktor | 90 [-] Show Supplier Material materials with Verlustfaktor of 90 [-] | dry | IEC 62631-2-1 | 100Hz |
190 [-] Show Supplier Material materials with Verlustfaktor of 190 [-] | dry | IEC 62631-2-1 | 1MHz | |
1000 [-] Show Supplier Material materials with Verlustfaktor of 1000 [-] | conditioned | IEC 62631-2-1 | 1MHz | |
3000 [-] Show Supplier Material materials with Verlustfaktor of 3000 [-] | conditioned | IEC 62631-2-1 | 100Hz | |
Volume resistivity | 1e+11 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+11 Ω·cm | conditioned | IEC 62631-3-1 | |
1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 62631-3-1 |
Rheological Properties
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Density of melt | 1160 g/cm³ Show Supplier Material materials with Density of melt of 1160 g/cm³ | dry | - | |
Schrumpfung | 0.6 % Show Supplier Material materials with Schrumpfung of 0.6 % | dry | ISO 294-4 | Parallel |
1 % Show Supplier Material materials with Schrumpfung of 1 % | dry | ISO 294-4 | Normal | |
Specific heat capacity melt | 2190 J/(kg·K) Show Supplier Material materials with Specific heat capacity melt of 2190 J/(kg·K) | dry | - | |
Thermal conductivity of melt | 0.33 W/(m·K) Show Supplier Material materials with Thermal conductivity of melt of 0.33 W/(m·K) | dry | - |
Technological properties
Property | ||
---|---|---|
Application areas | Molded case circuit breakers | |
Certifications | Yellow Card Available | |
Fillers | 25% Glass Fiber and Mineral Powder |