Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 1.54 g/cm³ Show Supplier Material materials with Dichte of 1.54 g/cm³ | dry | ISO 1183 |
Moisture absorption | 1.5 % Show Supplier Material materials with Moisture absorption of 1.5 % | dry | Sim. to ISO 62 |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Biegemodul | 6 GPa Show Supplier Material materials with Biegemodul of 6 GPa | conditioned | ISO 178 | |
7.7 GPa Show Supplier Material materials with Biegemodul of 7.7 GPa | dry | ISO 178 | ||
Dehnung | 2.1 % Show Supplier Material materials with Dehnung of 2.1 % | dry | ISO 527-1/-2 | |
Elastizitätsmodul | 9.2 GPa Show Supplier Material materials with Elastizitätsmodul of 9.2 GPa | dry | ISO 527-1/-2 | |
Flexural yield strength | 165 MPa Show Supplier Material materials with Flexural yield strength of 165 MPa | conditioned | ISO 178 | |
205 MPa Show Supplier Material materials with Flexural yield strength of 205 MPa | dry | ISO 178 | ||
Schlagfestigkeit, Charpy gekerbt | 23 °C | 9 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 9 kJ/m² | dry | ISO 179/1eA |
23 °C | 11 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 11 kJ/m² | conditioned | ISO 179/1eA | |
Schlagzähigkeit, Charpy ungekerbt | 23 °C | 38 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 38 kJ/m² | dry | ISO 179/1eU |
23 °C | 55.0 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 55.0 kJ/m² | conditioned | ISO 179/1eU | |
Zugfestigkeit | 135 MPa Show Supplier Material materials with Zugfestigkeit of 135 MPa | dry | ISO 527-1/-2 |
Thermisch
Property | Value | Condition | Testing Standard | Thickness | Pressure | Comment |
---|---|---|---|---|---|---|
Koeffizient der thermischen Ausdehnung | 3e-07 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 3e-07 1/K | dry | ISO 11359-1/-2 | Parallel | ||
7e-07 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 7e-07 1/K | dry | ISO 11359-1/-2 | Normal | |||
Relative temperature index, electrical | 65 °C Show Supplier Material materials with Relative temperature index, electrical of 65 °C | dry | UL746B | 0.75 mm | ||
Relative temperature index, mechanical impact | 65 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 65 °C | dry | UL746B | 0.75 mm | ||
Relative temperature index, mechanical strength | 65 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 65 °C | dry | UL746B | 0.75 mm | ||
Schmelzpunkt | 220 °C Show Supplier Material materials with Schmelzpunkt of 220 °C | dry | ISO 11357-1/-3 | 10°C/min | ||
Wärmeformbeständigkeitstemperatur | 205 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 205 °C | dry | ISO 75-1/-2 | 2 MPa | ||
220 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 220 °C | dry | ISO 75-1/-2 | 0.45 MPa |
Elektrisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Dielektrizitätskonstante | 4 [-] Show Supplier Material materials with Dielektrizitätskonstante of 4 [-] | dry | IEC 62631-2-1 | 1MHz |
Durchschlagfestigkeit | 23 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 23 kV/mm | dry | IEC 60243-1 | |
Kriechstromfestigkeit | 225 V Show Supplier Material materials with Kriechstromfestigkeit of 225 V | dry | IEC 60112 | |
Surface resistivity | 8e+12 Ω/sq Show Supplier Material materials with Surface resistivity of 8e+12 Ω/sq | conditioned | IEC 62631-3-2 | |
Verlustfaktor | 200 [-] Show Supplier Material materials with Verlustfaktor of 200 [-] | dry | IEC 62631-2-1 | 1MHz |
Volume resistivity | 8e+12 Ω·cm Show Supplier Material materials with Volume resistivity of 8e+12 Ω·cm | dry | IEC 62631-3-1 |
Rheological Properties
Technological properties
Property | ||
---|---|---|
Fillers | 20% Glass Fiber |