Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 1.2 g/cm³ Show Supplier Material materials with Dichte of 1.2 g/cm³ | dry | ISO 1183 |
Moisture absorption | 0.2 % Show Supplier Material materials with Moisture absorption of 0.2 % | dry | Sim. to ISO 62 |
Wasserabsorption | 0.65 % Show Supplier Material materials with Wasserabsorption of 0.65 % | dry | Sim. to ISO 62 |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Biegemodul | 0.18 GPa Show Supplier Material materials with Biegemodul of 0.18 GPa | dry | ISO 178 | ||
Dehnung | 300 % Show Supplier Material materials with Dehnung of 300 % | dry | ISO 527-1/-2 | ||
420 % Show Supplier Material materials with Dehnung of 420 % | dry | ISO 527-1/-2 | |||
820 % Show Supplier Material materials with Dehnung of 820 % | dry | ISO 527-1/-2 | |||
Elastizitätsmodul | 0.17 GPa Show Supplier Material materials with Elastizitätsmodul of 0.17 GPa | dry | ISO 527-1/-2 | ||
Elongation at yield | 20 % Show Supplier Material materials with Elongation at yield of 20 % | dry | ISO 527-1/-2 | ||
Härte, Shore D | 52 [-] Show Supplier Material materials with Härte, Shore D of 52 [-] | dry | ISO 868 | 3s | |
Reißfestigkeit | 125 kN/m Show Supplier Material materials with Reißfestigkeit of 125 kN/m | dry | ISO 34-1; Method B | ||
134 kN/m Show Supplier Material materials with Reißfestigkeit of 134 kN/m | dry | ISO 34-1; Method B | |||
Schlagfestigkeit, Charpy gekerbt | -30 °C | 25 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 25 kJ/m² | dry | ISO 179/1eA | |
Zugfestigkeit | 41 MPa Show Supplier Material materials with Zugfestigkeit of 41 MPa | dry | ISO 527-1/-2 | Normal |
Thermisch
Property | Value | Condition | Thickness | Testing Standard | Comment |
---|---|---|---|---|---|
Entflammbarkeit | HB | dry | 1.5 mm | IEC 60695-11-10 | UL recognition :Yes |
Koeffizient der thermischen Ausdehnung | 1.5e-06 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.5e-06 1/K | dry | ISO 11359-1/-2 | Parallel | |
1.5e-06 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.5e-06 1/K | dry | ISO 11359-1/-2 | Normal | ||
Relative temperature index, electrical | 50 °C Show Supplier Material materials with Relative temperature index, electrical of 50 °C | dry | 2 mm | UL746B | |
Relative temperature index, mechanical impact | 50 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 50 °C | dry | 2 mm | UL746B | |
Relative temperature index, mechanical strength | 50 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 50 °C | dry | 2 mm | UL746B | |
Schmelzpunkt | 207 °C Show Supplier Material materials with Schmelzpunkt of 207 °C | dry | ISO 11357-1/-3 | 10°C/min | |
Vicat-Erweichungstemperatur | 90 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 90 °C | dry | ISO 306 | 50°C/h 50N |
Elektrisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Dielektrizitätskonstante | 4 [-] Show Supplier Material materials with Dielektrizitätskonstante of 4 [-] | dry | IEC 62631-2-1 | 1MHz |
4.4 [-] Show Supplier Material materials with Dielektrizitätskonstante of 4.4 [-] | dry | IEC 62631-2-1 | 100Hz | |
Durchschlagfestigkeit | 21 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 21 kV/mm | dry | IEC 60243-1 | |
Verlustfaktor | 400 [-] Show Supplier Material materials with Verlustfaktor of 400 [-] | dry | IEC 62631-2-1 | 1MHz |
Volume resistivity | 1e+11 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+11 Ω·cm | dry | IEC 62631-3-1 |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Schmelzvolumenflussrate | 230 °C | 9 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 9 cm³/10min | dry | ISO 1133 |
Technological properties
Property | ||
---|---|---|
Application areas | Seat Suspension/Fabrics, Railway Buffers, Truck Trailer Power and Signal Cord, Power transmission belts, Industrial Cords and Ropes | |
Certifications | Food Contact, Yellow Card Available |