Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 1.21 g/cm³ Show Supplier Material materials with Dichte of 1.21 g/cm³ | dry | ISO 1183 |
Mechanisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Dehnung | 205 % Show Supplier Material materials with Dehnung of 205 % | dry | ISO 527-1/-2 | |
Elastizitätsmodul | 0.12 GPa Show Supplier Material materials with Elastizitätsmodul of 0.12 GPa | dry | ISO 527-1/-2 | |
Härte, Shore D | 45 [-] Show Supplier Material materials with Härte, Shore D of 45 [-] | dry | ISO 868 | 3s |
Zugfestigkeit | 19.5 MPa Show Supplier Material materials with Zugfestigkeit of 19.5 MPa | dry | ISO 527-1/-2 |
Thermisch
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Schmelzvolumenflussrate | 230 °C | 9.6 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 9.6 cm³/10min | dry | ISO 1133 |
Technological properties
Property |
---|