Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 0.65 g/cm³ Show Supplier Material materials with Dichte of 0.65 g/cm³ | dry | ISO 60 |
1.09 g/cm³ Show Supplier Material materials with Dichte of 1.09 g/cm³ | dry | ISO 1183 | |
Wasserabsorption | 0.8 % Show Supplier Material materials with Wasserabsorption of 0.8 % | dry | Sim. to ISO 62 |
Mechanisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Dehnung | 300 % Show Supplier Material materials with Dehnung of 300 % | dry | ISO 527-1/-2 | |
500 % Show Supplier Material materials with Dehnung of 500 % | dry | ISO 527-1/-2 | ||
Elastizitätsmodul | 0.02 GPa Show Supplier Material materials with Elastizitätsmodul of 0.02 GPa | dry | ISO 527-1/-2 | |
Härte, Shore A | 85 [-] Show Supplier Material materials with Härte, Shore A of 85 [-] | dry | ISO 868 | 3s |
Härte, Shore D | 25 [-] Show Supplier Material materials with Härte, Shore D of 25 [-] | dry | ISO 868 | 3s |
Zugfestigkeit | 11 MPa Show Supplier Material materials with Zugfestigkeit of 11 MPa | dry | ISO 527-1/-2 |
Thermisch
Property | Value | Condition | Thickness | Testing Standard | Comment |
---|---|---|---|---|---|
Entflammbarkeit | HB | dry | 1.5 mm | IEC 60695-11-10 | UL recognition :Yes |
Glasübergangstemperatur | -80 °C Show Supplier Material materials with Glasübergangstemperatur of -80 °C | dry | ISO 11357-1/-2 | 10°C/min | |
-74 °C Show Supplier Material materials with Glasübergangstemperatur of -74 °C | dry | ASTM D5026/D7028 | DMTA (tan d) | ||
Koeffizient der thermischen Ausdehnung | 2.2e-06 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 2.2e-06 1/K | dry | ISO 11359-1/-2 | Parallel | |
2.2e-06 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 2.2e-06 1/K | dry | ISO 11359-1/-2 | Normal | ||
Relative temperature index, electrical | 50 °C Show Supplier Material materials with Relative temperature index, electrical of 50 °C | dry | 2 mm | UL746B | |
Relative temperature index, mechanical impact | 50 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 50 °C | dry | 2 mm | UL746B | |
Relative temperature index, mechanical strength | 50 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 50 °C | dry | 2 mm | UL746B | |
Schmelzpunkt | 180 °C Show Supplier Material materials with Schmelzpunkt of 180 °C | dry | ISO 11357-1/-3 | 10°C/min |
Elektrisch
Property | Value | Condition | Testing Standard |
---|---|---|---|
Volume resistivity | 5e+12 Ω·cm Show Supplier Material materials with Volume resistivity of 5e+12 Ω·cm | dry | IEC 62631-3-1 |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Density of melt | 905 g/cm³ Show Supplier Material materials with Density of melt of 905 g/cm³ | dry | - | ||
Schmelzvolumenflussrate | 230 °C | 48 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 48 cm³/10min | dry | ISO 1133 | |
Schrumpfung | 1 % Show Supplier Material materials with Schrumpfung of 1 % | dry | Sim. to ISO 294-4 | Parallel | |
1 % Show Supplier Material materials with Schrumpfung of 1 % | dry | Sim. to ISO 294-4 | Normal |
Technological properties
Property | ||
---|---|---|
Certifications | Yellow Card Available |