Allgemein
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Bio-based content | 43 % Show Supplier Material materials with Bio-based content of 43 % | dry | ASTM D6866-12 Method B | |
Dichte | 1.14 g/cm³ Show Supplier Material materials with Dichte of 1.14 g/cm³ | dry | ISO 1183 | |
Moisture absorption | 0.03 % Show Supplier Material materials with Moisture absorption of 0.03 % | dry | Sim. to ISO 62 | |
Wasserabsorption | 0.14 % Show Supplier Material materials with Wasserabsorption of 0.14 % | dry | ISO 62 | at 23°C after 24h |
Mechanisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Biegemodul | 0.1 GPa Show Supplier Material materials with Biegemodul of 0.1 GPa | dry | ISO 178 | |
Dehnung | 250 % Show Supplier Material materials with Dehnung of 250 % | dry | ISO 527-1/-2 | |
700 % Show Supplier Material materials with Dehnung of 700 % | dry | ISO 527-1/-2 | ||
Elastizitätsmodul | 0.09 GPa Show Supplier Material materials with Elastizitätsmodul of 0.09 GPa | dry | ISO 527-1/-2 | |
Härte, Shore D | 45 [-] Show Supplier Material materials with Härte, Shore D of 45 [-] | dry | ISO 868 | 3s |
Reißfestigkeit | 106 kN/m Show Supplier Material materials with Reißfestigkeit of 106 kN/m | dry | ISO 34-1; Method B | |
107 kN/m Show Supplier Material materials with Reißfestigkeit of 107 kN/m | dry | ISO 34-1; Method B | ||
Zugfestigkeit | 17 MPa Show Supplier Material materials with Zugfestigkeit of 17 MPa | dry | ISO 527-1/-2 | |
24 MPa Show Supplier Material materials with Zugfestigkeit of 24 MPa | dry | ISO 527-1/-2 | Normal |
Thermisch
Elektrisch
Property | Value | Condition | Testing Standard |
---|---|---|---|
Durchschlagfestigkeit | 20 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 20 kV/mm | dry | IEC 60243-1 |
Surface resistivity | 1e+15 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+15 Ω/sq | dry | IEC 62631-3-2 |
Volume resistivity | 1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 62631-3-1 |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Schmelzvolumenflussrate | 230 °C | 39 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 39 cm³/10min | dry | ISO 1133 | |
Schrumpfung | 1.3 % Show Supplier Material materials with Schrumpfung of 1.3 % | dry | ISO 294-4 | Parallel | |
1.3 % Show Supplier Material materials with Schrumpfung of 1.3 % | dry | Sim. to ISO 294-4 | Parallel | ||
1.5 % Show Supplier Material materials with Schrumpfung of 1.5 % | dry | ISO 294-4 | Normal | ||
1.5 % Show Supplier Material materials with Schrumpfung of 1.5 % | dry | Sim. to ISO 294-4 | Normal |
Technological properties
Property | ||
---|---|---|
Application areas | Smokable Sausage Casings, Phone case | |
Certifications | Food Contact, Yellow Card Available |