Allgemein
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Dichte | 1.23 g/cm³ Show Supplier Material materials with Dichte of 1.23 g/cm³ | dry | ISO 1183 | |
Moisture absorption | 3.2 % Show Supplier Material materials with Moisture absorption of 3.2 % | dry | Sim. to ISO 62 | |
Wasserabsorption | 3.2 % Show Supplier Material materials with Wasserabsorption of 3.2 % | dry | ISO 62 | at 23°C after 24h |
11.5 % Show Supplier Material materials with Wasserabsorption of 11.5 % | dry | Sim. to ISO 62 |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Biegemodul | 5.8 GPa Show Supplier Material materials with Biegemodul of 5.8 GPa | conditioned | ISO 178 | |
11.5 GPa Show Supplier Material materials with Biegemodul of 11.5 GPa | dry | ISO 178 | ||
Dehnung | 2.3 % Show Supplier Material materials with Dehnung of 2.3 % | dry | ISO 527-1/-2 | |
4 % Show Supplier Material materials with Dehnung of 4 % | conditioned | ISO 527-1/-2 | ||
Elastizitätsmodul | 13 GPa Show Supplier Material materials with Elastizitätsmodul of 13 GPa | dry | ISO 527-1/-2 | |
Flexural yield strength | 150 MPa Show Supplier Material materials with Flexural yield strength of 150 MPa | conditioned | ISO 178 | |
280 MPa Show Supplier Material materials with Flexural yield strength of 280 MPa | dry | ISO 178 | ||
Schlagfestigkeit, Charpy gekerbt | 23 °C | 5.5 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 5.5 kJ/m² | dry | ISO 179/1eA |
Zugfestigkeit | 120 MPa Show Supplier Material materials with Zugfestigkeit of 120 MPa | conditioned | ISO 527-1/-2 | |
200 MPa Show Supplier Material materials with Zugfestigkeit of 200 MPa | dry | ISO 527-1/-2 |
Thermisch
Property | Value | Condition | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|
Glasübergangstemperatur | 75 °C Show Supplier Material materials with Glasübergangstemperatur of 75 °C | dry | ISO 11357-1/-2 | 10°C/min | |
Koeffizient der thermischen Ausdehnung | 2.5e-07 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 2.5e-07 1/K | dry | ISO 11359-1/-2 | Parallel | |
5e-07 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 5e-07 1/K | dry | ISO 11359-1/-2 | Normal | ||
Schmelzpunkt | 295 °C Show Supplier Material materials with Schmelzpunkt of 295 °C | dry | ISO 11357-1/-3 | 10°C/min | |
Wärmeformbeständigkeitstemperatur | 290 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 290 °C | dry | ISO 75-1/-2 | 2 MPa |
Technological properties
Property | ||
---|---|---|
Certifications | Yellow Card Available | |
Fillers | 15% Carbon Fiber |