Allgemein
Property | Value | Condition | Testing Standard |
---|---|---|---|
Dichte | 1.41 g/cm³ Show Supplier Material materials with Dichte of 1.41 g/cm³ | dry | ISO 1183 |
Moisture absorption | 1.8 % Show Supplier Material materials with Moisture absorption of 1.8 % | dry | Sim. to ISO 62 |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard |
---|---|---|---|---|
Biegemodul | 6.8 GPa Show Supplier Material materials with Biegemodul of 6.8 GPa | conditioned | ISO 178 | |
9.8 GPa Show Supplier Material materials with Biegemodul of 9.8 GPa | dry | ISO 178 | ||
Dehnung | 2.6 % Show Supplier Material materials with Dehnung of 2.6 % | dry | ISO 527-1/-2 | |
5 % Show Supplier Material materials with Dehnung of 5 % | conditioned | ISO 527-1/-2 | ||
Elastizitätsmodul | 6.7 GPa Show Supplier Material materials with Elastizitätsmodul of 6.7 GPa | conditioned | ISO 527-1/-2 | |
11.4 GPa Show Supplier Material materials with Elastizitätsmodul of 11.4 GPa | dry | ISO 527-1/-2 | ||
Flexural yield strength | 200 MPa Show Supplier Material materials with Flexural yield strength of 200 MPa | conditioned | ISO 178 | |
295 MPa Show Supplier Material materials with Flexural yield strength of 295 MPa | dry | ISO 178 | ||
Schlagfestigkeit, Charpy gekerbt | 23 °C | 14.0 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 14.0 kJ/m² | dry | ISO 179/1eA |
23 °C | 24 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 24 kJ/m² | conditioned | ISO 179/1eA | |
Schlagzähigkeit, Charpy ungekerbt | 23 °C | 96 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 96 kJ/m² | dry | ISO 179/1eU |
23 °C | 100 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 100 kJ/m² | conditioned | ISO 179/1eU | |
Zugfestigkeit | 125 MPa Show Supplier Material materials with Zugfestigkeit of 125 MPa | conditioned | ISO 527-1/-2 | |
190 MPa Show Supplier Material materials with Zugfestigkeit of 190 MPa | dry | ISO 527-1/-2 |
Thermisch
Property | Value | Condition | Testing Standard | Pressure | Comment |
---|---|---|---|---|---|
Schmelzpunkt | 220 °C Show Supplier Material materials with Schmelzpunkt of 220 °C | dry | ISO 11357-1/-3 | 10°C/min | |
Wärmeformbeständigkeitstemperatur | 206 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 206 °C | dry | ISO 75-1/-2 | 2 MPa | |
220 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 220 °C | dry | ISO 75-1/-2 | 0.45 MPa |
Elektrisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Dielektrizitätskonstante | 4 [-] Show Supplier Material materials with Dielektrizitätskonstante of 4 [-] | dry | IEC 62631-2-1 | 100Hz |
4 [-] Show Supplier Material materials with Dielektrizitätskonstante of 4 [-] | dry | IEC 62631-2-1 | 1MHz | |
Durchschlagfestigkeit | 23 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 23 kV/mm | dry | IEC 60243-1 | |
Kriechstromfestigkeit | 400 V Show Supplier Material materials with Kriechstromfestigkeit of 400 V | dry | IEC 60112 | |
Surface resistivity | 3e+13 Ω/sq Show Supplier Material materials with Surface resistivity of 3e+13 Ω/sq | conditioned | IEC 62631-3-2 | |
Verlustfaktor | 110 [-] Show Supplier Material materials with Verlustfaktor of 110 [-] | dry | IEC 62631-2-1 | 100Hz |
190 [-] Show Supplier Material materials with Verlustfaktor of 190 [-] | dry | IEC 62631-2-1 | 1MHz | |
Volume resistivity | 7e+12 Ω·cm Show Supplier Material materials with Volume resistivity of 7e+12 Ω·cm | dry | IEC 62631-3-1 |
Rheological Properties
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Schmelzmassenflussrate | 250 °C | 4 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 4 g/10min | dry | ISO 1133 | |
Schmelzvolumenflussrate | 250 °C | 3 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 3 cm³/10min | dry | ISO 1133 | |
Schrumpfung | 0.3 % Show Supplier Material materials with Schrumpfung of 0.3 % | dry | ISO 294-4 | Parallel | |
1 % Show Supplier Material materials with Schrumpfung of 1 % | dry | ISO 294-4 | Normal |
Technological properties
Property | ||
---|---|---|
Certifications | Yellow Card Available | |
Fillers | 35% Glass Fiber |